H.C. Starck Amperit® 421.1 NiCoCrAlTaReY (MCrAlY)

Category Metal , Nonferrous Metal , Nickel Alloy
Manufacturer H.C. Starck
Trade Name Amperit®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Amperit® 421.1 NiCoCrAlTaReY (MCrAlY).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Particle Size 22 µm
22 µm
Maximum of 15% less than
45 µm
45 µm
Maximum of 7% greater than
Component Elements Properties Metric English Comments
Aluminum, Al 6.25 - 6.75 %
6.25 - 6.75 %
Chromium, Cr 17 - 19 %
17 - 19 %
Cobalt, Co 9.0 - 11 %
9.0 - 11 %
Hafnium, Hf 0.40 - 0.60 %
0.40 - 0.60 %
Nickel, Ni 52.6 - 58.8 %
52.6 - 58.8 %
Rhenium, Re 1.8 - 2.2 %
1.8 - 2.2 %
Silicon, Si 0.80 - 1.2 %
0.80 - 1.2 %
Tantalum, Ta 5.75 - 6.25 %
5.75 - 6.25 %
Yttrium, Y 0.20 - 0.40 %
0.20 - 0.40 %