H.C. Starck Amperit® 512.074 Agglomerated Sintered Tungsten Carbide - Cobalt (WC-Co) 88-12

Category Ceramic , Carbide
Manufacturer H.C. Starck
Trade Name Amperit®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Amperit® 512.074 Agglomerated Sintered Tungsten Carbide - Cobalt (WC-Co) 88-12.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 3.80 - 4.50 g/cc
0.137 - 0.163 lb/in³
ASTM B212
Particle Size 17 - 21 µm
17 - 21 µm
10%
30 - 38 µm
30 - 38 µm
50%
53 - 63 µm
53 - 63 µm
90%
<= 89 µm
<= 89 µm
100% less than
Component Elements Properties Metric English Comments
Carbon, C 3.9 - 4.6 %
3.9 - 4.6 %
Cobalt, Co 10 - 12 %
10 - 12 %
Iron, Fe <= 0.30 %
<= 0.30 %