H.C. Starck Amperit® 742.1 Aluminum Oxide-Titanium Oxide 97-3 (Al2O3-TiO2)

Category Ceramic , Oxide , Aluminum Oxide
Manufacturer H.C. Starck
Trade Name Amperit®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Amperit® 742.1 Aluminum Oxide-Titanium Oxide 97-3 (Al2O3-TiO2).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Particle Size 15 µm
15 µm
Maximum of 5% less than
62 µm
62 µm
Minimum of 95% less than
88 µm
88 µm
100% less than
Component Elements Properties Metric English Comments
Al2O3 95.4 - 98 %
95.4 - 98 %
Fe2O3 <= 0.50 %
<= 0.50 %
SiO2 <= 0.60 %
<= 0.60 %
TiO2 2.0 - 3.5 %
2.0 - 3.5 %