H.C. Starck Grade A Zirconium Diboride, ZrB2

Category Ceramic , Boride
Manufacturer H.C. Starck
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF H.C. Starck Grade A Zirconium Diboride, ZrB2.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Hot-pressed composites of excellent electrical conductivity, e.g., evaporation boats for continuous aluminum metallizingCrucible material for non-ferrous metalsCeramic shapes to be used in production of Al in Hall-Heroult cellsHot pressed TiB, armor platesCutting tools and cermets, suitable for machining aluminumMetal Matrix CompositesAntioxidant in carbon-bonded refractoriesBurnable absorbers for neutrons
Physical Properties Metric English Comments
Particle Size 3.0 - 5.0 µm
3.0 - 5.0 µm
Average Particle Size/Laser Diffraction D50
<= 12 µm
<= 12 µm
90% less than
Component Elements Properties Metric English Comments
Hafnium, Hf >= 0.20 %
>= 0.20 %