Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Size | >= 3.0 µm | >= 3.0 µm | 10% smaller than |
Nyco NYAD® M325 Wollastonite Powdered grade.Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance m.. |
|||
Particle Size | >= 3.0 µm | >= 3.0 µm | 10% smaller than |
Nyco RRIMGLOS® 4W Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Particle Size | 3.0 µm | 3.0 µm | Median Grain Diameter |
Nabaltec APYMAG® 80 Magnesium Hydroxide The demand for halogen free flame retardant plastics for applications in automobile, electrical, and construction industries is stronger than ever. The use of mineral flame retardants within these p.. |
|||
Particle Size | 3.0 µm | 3.0 µm | Median Grain Diameter |
Nabaltec NABALOX® NO 113 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Particle Size | 3.0 µm | 3.0 µm | Median Grain Diameter |
Nabaltec NABALOX® NO 315 Ground Alumina NABALOX® aluminum oxide has a number of advantages including low sintering temperaturewide sintering rangeflexible processinghigh sintered densities high wear and impact resistanceelectrical insula.. |
|||
Particle Size | <= 3.0 µm | <= 3.0 µm | Best Grade |
Oceanchem Group Decabromodiphenyl Ethane (DBDPE/8010) Molecular Formula: C14Br10H4Cas No.: 84852-53-9Characteristics: White powder, no poison, no smell and noncorrosion. Indissolvable in water, ethyl alcohol, acetone, benzene, arene chloride.Use: This.. |
|||
Particle Size | 3.0 - 5.0 µm | 3.0 - 5.0 µm | First Grade |
Oceanchem Group Zinc Borate Information Provided by Oceanchem Group |
|||
Particle Size | 3.0 µm | 3.0 µm | 50% of particles, (RWG Powder) |
Ferro IP 780 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | 3.0 µm | 3.0 µm | 50% of particles, (RWG Powder) |
Ferro IP 820 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | 3.0 µm | 3.0 µm | d90 |
Magyar Aluminum ALO-DN-7P Alumina Ground Alumina |
|||
Particle Size | 3.0 µm | 3.0 µm | d90 |
Magyar Aluminum ALO-EL-7P Alumina Ground Alumina |
|||
Particle Size | 3.0 - 6.0 µm | 3.0 - 6.0 µm | d50 |
Magyar Aluminum ALOLT 50AF Aluminum Hydroxide Ground type |
|||
Particle Size | 3.0 - 5.0 µm | 3.0 - 5.0 µm | average |
Malvern Minerals Novakup® L-207A Surface-Treated Lamellar Quartz Filler/Extender Novakup® is a surface modified or silane treated Novacite®. It has been used its barrier prosperities in chemical and corrosion resistant applications and as a filler/extender/reinforcing agen.. |
|||
Particle Size | 3.0 - 4.0 µm | 3.0 - 4.0 µm | Average |
Malvern Minerals Trikup® PF Silane Treated Aluminum Hydroxide Trikup® is a custom, silane treated alumina trihydrate or aluminum hydroxide. ATH is the largest volume flame retardant in the world. Trikup® adds additional functionality through the use of .. |
|||
Particle Size | 3.0 µm | 3.0 µm | mean |
Imerys Minsparâ„¢ 10 Ground Feldspar Minsparâ„¢ 10 is a fine particle size, ground Feldspar with a tightly controlled particle size distribution. Minsparâ„¢ 10 is easily dispersed to a high Hegman grind to produce coatings finish.. |
|||
Particle Size | 3.0 µm | 3.0 µm | 50% |
Minelco UltraCarb LH15C-10 Hydrated Magnesium Calcium Carbonate Mineral Flame RetardantUltracarb combines properties normally associated with several different materials that can be used jointly or individually to benefit many applications including rubber, plas.. |
|||
Particle Size | 3.0 µm | 3.0 µm | 50% |
Minelco UltraCarb LH15X Hydrated Magnesium Calcium Carbonate Mineral Flame RetardantUltracarb combines properties normally associated with several different materials that can be used jointly or individually to benefit many applications including rubber, plas.. |
|||
Particle Size | 3.0 µm | 3.0 µm | Crystal Size |
Momentive Performance Materials HCPH Boron Nitride (BN) Powder GE Advanced Ceramics boron nitride (BN) powders of grades HCP, HCPH, HCPL, and AC6004 are generally single-crystal hexagonal platelets with very high purity. The mean particle sizes for these ultra-.. |
|||
Particle Size | 3.0 - 6.0 µm | 3.0 - 6.0 µm | mean; 100% -325 mesh |
Momentive Performance Materials HCT-F Titanium Diboride (TiB2) Powder Grade HCT-F powders are designed for use on applications requiring reduced particle size without sacrificing high purity.Titanium Diboride Powder Titanium Diboride (TiB2) is produced by GE Advanced.. |
|||
Particle Size | 3.0 - 5.0 µm | 3.0 - 5.0 µm | Laser Diffraction D50 |
H.C. Starck Grade B Zirconium Carbide, ZrC Additive for hard metalsAdditive for powder metallurgyModerator in solid fuel propellant |
|||
Particle Size | 3.0 µm | 3.0 µm | 50% of particles, (RWG Powder) |
Ferro IP 730 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | 3.0 µm | 3.0 µm | 50% of particles, (RWG Powder) |
Ferro IP 745 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-B-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to.. |
|||
Particle Size | 3.0 µm | 3.0 µm | 50% of particles, (RWG Powder) |
Ferro IP 770 Passivation Glasses (Pb-B-Si-Al; Pb-Si-Al; Si-Pb-Al Silicates) Glass Type: Pb-Si-Al Typical Powder Form: TF, REG, RWG, SRRG Ferro's passivation glasses are designed for use on transistors, thyristors, and diodes. These products are formulated and produced to a.. |
|||
Particle Size | 3.0 - 5.0 µm | 3.0 - 5.0 µm | Median Grain (d50) |
CeramTec Rubalit® 708S Alumina, 96% Rubalit® 708S (96%) is an alumina that features high strength and thermal conductivity. It provides outstanding results when used on commercially available thick-film pastes and metallization syste.. |
|||
Particle Size | 3.0 - 4.0 µm | 3.0 - 4.0 µm | |
Dow Corning EP-9261 TI Cosmetic Powder This cosmetic powder provides smoothness and a powdery, non-greasy skin feel; high sebum absorption; soft focus; and improves SPF. As a white cross-linked dimethyl polysiloxane elastomer powder comb.. |
|||
Particle Size | 3.0 µm | 3.0 µm | Median |
Excalibar ExBar™ W 3 Barite BaSO4 Powder ExBar™ W high-purity white barytes are manufactured using only the highest quality white, natural barium sulfate ore. Strict quality control results in consistent products that are used in paints, .. |
|||
Particle Size | 3.0 µm | 3.0 µm | D50 |
Dandong Taico Minerals TAICOCITE® TC35 Magnesium Hydroxide Made from local natural brucite minerals, TAICOCITE® is the name of milled magnesium hydroxide products which is produced (micronized/surface treated) by Dandong Taico Minerals Co., Ltd. TAICOCITE®.. |
|||
Particle Size | 3.0 - 5.0 µm | 3.0 - 5.0 µm | median, milled |
ATI Wah Chang Hafnium Oxide, HfO2 A free flowing, coarse, tan powder.Information provided by ATI Wah ChangTypical Analysis: On Hf metal basis |
|||
Particle Size | 3.0 - 5.0 µm | 3.0 - 5.0 µm | Medium Grain (d50) |
CeramTec CeramCool® Rubalit® 708 Alumina, 96% CeramCool® is a metallized ceramic heat-sink for high power applications demonstrated by high power LED-systems. CeramCool® material characteristics: electrical insulation, high volume resistivit.. |
|||
Particle Size | >= 3.0 µm | >= 3.0 µm | D10 |
Potters Industries A-Series Z-CEL® 8054 White Synthetic Sodium Aluminosilicate Microsphere Fine particle white spheres developed as filler for paints, coatings and films.Information provided by Potters Industries. |