Material Notes:
Poly(3,4-ethylenedioxythiophene)poly(styrenesulfonate), provided as an aqueous dispersion used to produce thin film antistatic coatings. Clevios™ P Jet HC V2 is an antistatic material based on PEDOT:PSS – chemistry for electronics applications. This conductive polymer is an inkjet formulation, acidic, high conductive version of Clevios™ P. Typical applications include the antistatic coating of PET or Polycarbonate films for antistatic trays and blister tapes, films for dust protection of components in the LCD industry, antistatic coating of glass, high quality antistatic-coated papers, and other ESD and dissipative applicationsInformation provided by Heraeus, Conductive Polymers Division.
Physical Properties Metric English Comments
Solids Content 0.60 - 1.2 %
0.60 - 1.2 %
As Supplied
Viscosity 5.0 - 20 cP

@Shear Rate 11.7 1/s
5.0 - 20 cP

@Shear Rate 11.7 1/s
As Supplied
Electrical Properties Metric English Comments
Electrical Resistivity 0.00330 ohm-cm
0.00330 ohm-cm
Processing Properties Metric English Comments
Shelf Life 6.00 Month

@Temperature 5.00 - 30.0 °C
6.00 Month

@Temperature 41.0 - 86.0 °F
in unopened original container
Descriptive Properties Value Comments
Form Supplied Blue Liquid