Material Notes:
HexPly® 8551-7 is an amine-cured, toughened epoxy resin system supplied with unidirectional graphite fibers. Typical reinforcement is continuous IM7 (intermediate modulus) graphite filaments. HexPly® 8551-7 was developed to operate in a temperature environment of up to 200°F (93°C). IM7/8551-7 is an extremely damage-resistant system, recommended for structural applications requiring high strength, stiffness, and damage tolerance. Conventional thermoset resin processing equipment and techniques can be used to process IM7/8551-7 prepreg tape.Features: Service temperature up to 200°F (93°C), Extremely damage-resistant system, 350°F (177°C)
Physical Properties Metric English Comments
Density 1.272 g/cc
0.04595 lb/in³
Moisture Absorption at Equilibrium 3.1 %
3.1 %
Viscosity 1900 cP

@Temperature 129 - 149 °C
1900 cP

@Temperature 264 - 300 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 99.3 MPa
14400 psi
Elongation at Yield 4.4 %
4.4 %
Tensile Modulus 4.09 GPa
593 ksi
Fracture Toughness 3.51 MPa-m½
3.19 ksi-in½
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 93.3 °C
200 °F
Glass Transition Temp, Tg 116 °C
241 °F
Wet
157 °C
315 °F
Dry
Processing Properties Metric English Comments
Gel Time 8.00 - 16.0 min

@Temperature 177 °C
8.00 - 16.0 min

@Temperature 351 °F
Descriptive Properties Value Comments
Tack Life (days) 40