Viscosity 1900 - 2100 cP
1900 - 2100 cP
Liquid State
Palm Labs Adhesives TURBO FUSE 2000CP FLUORESCENT Rapid Bonding Adhesive
Palm Lab's Cyanoacrylate is a one component rapid bonding adhesive. TURBO FUSE FLUORESCENT advanced formula is designed to polymerize instantly by absorbing surface moisture. The product's performan..
Viscosity 1900 cP

@Temperature 25.0 °C
1900 cP

@Temperature 77.0 °F
After mixing
Tra-Con Tra-Bond 2129 Clear Low Viscosity Epoxy Adhesive
TRA-BOND 2129 is a low viscosity epoxy adhesive recommended for industrial and electronic production, repair, small casting, coating, tooling, and rigid laminating applications where a clear system ..
Viscosity 1900 cP

@Temperature 25.0 °C
1900 cP

@Temperature 77.0 °F
Mixed (lv #4, 12 rpm)
Tra-Con Tra-Bond 526D01
Information provided by Tra-Con Inc.
Viscosity 1900 cP

@Temperature 129 - 149 °C
1900 cP

@Temperature 264 - 300 °F
Hexcel® HexPly® 8551-7 Epoxy Matrix
HexPly® 8551-7 is an amine-cured, toughened epoxy resin system supplied with unidirectional graphite fibers. Typical reinforcement is continuous IM7 (intermediate modulus) graphite filaments. HexPl..
Viscosity 1900 - 2900 cP
1900 - 2900 cP
Cone & Plate; ISO 3219 (93)
Dow SPECFLEX™ NC 606 Polyol
SPECFLEX™ NC 606 polyol is a co-polymer polyol especially designed for the production of High Resilience (HR) molded flexible foams. It processes well on all types of foam machinery. CAS# 00908..
Viscosity 1900 - 2900 cP

@Temperature 35.0 °C
1900 - 2900 cP

@Temperature 95.0 °F
C.O.I.M. UREXTER® T 400 Polyurethane Two-Component Compound
Description: Polyester PU System for shoe sole manufacturingInformation provided by P.A.T. Products, Inc.
Viscosity 1900 cP
1900 cP
A Component; Spindle #2; speed 10 rpm; ASTM D1824
Aptek 6100-1A/B Epoxy Encapsulant
Optoelectronic grade, water clear encapsulant for IR and visible LED discreet devices. Lower Tg versions available for display devices.Part A is dark blue. Part B is clear to pale yellow.Information..
Viscosity 1900 cP

@Temperature 177 °C
1900 cP

@Temperature 350 °F
Typical
Bostik 2391 Versatile, Good Hot Tack EVA Glue Stick
Bostik 2391 Versatile, Good Hot Tack EVA Glue StickVersatile packaging product. Good "hot tack."
Viscosity 1900 cP
1900 cP
Abatron AboCast 50-11/AboCure 50-4 Epoxy
AboCast 50-11 is a clear unfilled resin with low viscosity and a weight of 9.5 lbs/gallon. AboCure 50-4 is clear, slow converter with a variable ratio, low viscosity, and a weight of 8 lbs/gallon. A..
Viscosity 1900 cP
1900 cP
Mixed - low; Resin - 1,900 cP; Hardener - 2,800 cP
Loctite® Durabond® E-05CL Epoxy Adhesive