Material Notes:
HexPly® M21 is a new, very tough epoxy matrix that exhibits excellent damage tolerance, especially at high energy impact. It has been developed to meet the needs of the latest generation of primary aircraft structures and Formula 1 Grand Prix cars.HexPly® M21 benefits from easy processing as a result of controlled flow and a simple cure schedule. It is best suited to press or autoclave cure to obtain optimum mechanical performance from the cured composite.Information provided by HexCel
Physical Properties Metric English Comments
Density 1.28 g/cc
0.0462 lb/in³
Mechanical Properties Metric English Comments
Elongation at Yield 5.0 %
5.0 %
Flexural strain
Flexural Yield Strength 147 MPa
21300 psi
Flexural Modulus 3.50 GPa
508 ksi
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 185 °C
365 °F
Processing Properties Metric English Comments
Shelf Life >= 12.0 Month

@Temperature -18.0 °C
>= 12.0 Month

@Temperature -0.400 °F
Descriptive Properties Value Comments
Tack Life (days) 30