Hexcel® HexPly® M52 120°C/250°F Curing Epoxy, M52/40%/193P/CHS-3K

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Epoxy , Epoxy/Carbon Fiber Composite
Manufacturer Hexcel
Trade Name HexPly®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® M52 120°C/250°F Curing Epoxy, M52/40%/193P/CHS-3K.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fiber: HS Carbon, Plain Weave, 193 g/m2Information provided by HexCel
Physical Properties Metric English Comments
Density 1.20 g/cc
0.0434 lb/in³
Resin
1.49 g/cc
0.0538 lb/in³
Nominal Laminate
1.78 g/cc
0.0643 lb/in³
Fibre
Mechanical Properties Metric English Comments
Tensile Strength, Yield 751 MPa
109000 psi
EN2561
Tensile Modulus 63.8 GPa
9250 ksi
EN2561
Flexural Yield Strength 971 MPa
141000 psi
EN2562
Flexural Modulus 65.6 GPa
9510 ksi
EN2562
Compressive Yield Strength 604 MPa
87600 psi
EN2850B
Compressive Modulus 61.0 GPa
8850 ksi
EN2850B
Shear Strength 60.0 MPa
8700 psi
ILSS; EN2563
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 85.0 - 90.0 °C
185 - 194 °F
DMA Onset
Processing Properties Metric English Comments
Shelf Life 12.0 Month

@Temperature -18.0 °C
12.0 Month

@Temperature -0.400 °F
Descriptive Properties Value Comments
Cured Thickness per Ply (cm) 0.0216
Fiber Volume (%) 50.3