Material Notes:
Hard, stiff, very good impact properties with a wide range of temperature (to -100°C). High stability of shape under heat. Clear with own slight yellowish color. Low water absorption, weather-resistant. Physiologically acceptable.Information provided by Hippe.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
DIN 53 479
Moisture Absorption at Equilibrium 0.15 %
0.15 %
Absorption of humidity in standard operating environment; DIN 53 715
Water Absorption at Saturation 0.35 %
0.35 %
DIN 53 495
Mechanical Properties Metric English Comments
Ball Indentation Hardness 100 MPa

@Time 30.0 sec
14500 psi

@Time 0.00833 hour
DIN 53 456
Tensile Strength 65.0 MPa
9430 psi
DIN 53 455
Elongation at Break 60 - 100 %
60 - 100 %
DIN 53 455
Tensile Modulus 2.20 GPa
319 ksi
DIN 53 457
Charpy Impact, Notched NB
NB
DIN 53 453
Coefficient of Friction, Dynamic 0.52 - 0.58
0.52 - 0.58
Against steel, p=0.05 N/mm², v=0.6 m/s, hardened and ground
Abrasion 22
22
µm/km; Against steel, p=0.05 N/mm², v=0.6 m/s, hardened and ground
Thermal Properties Metric English Comments
CTE, linear 60.0 - 70.0 µm/m-°C
33.3 - 38.9 µin/in-°F
Specific Heat Capacity 1.20 J/g-°C
0.287 BTU/lb-°F
Thermal Conductivity 0.190 W/m-K
1.32 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 120 °C
248 °F
Continuous use
140 °C
284 °F
Short Periods
Deflection Temperature at 0.46 MPa (66 psi) 140 °C
284 °F
ISO-R 75 Method B
Deflection Temperature at 1.8 MPa (264 psi) 135 °C
275 °F
ISO-R 75 Method A
Glass Transition Temp, Tg 145 °C
293 °F
dynamic; DIN 53 736
Flammability, UL94 V-2
V-2
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+17 ohm-cm
1.00e+17 ohm-cm
DIN 53 482, VDE 0303, Part 3
Surface Resistance 1.00e+15 ohm
1.00e+15 ohm
DIN 53 482
Dielectric Constant 3.0

@Frequency 1.00e+6 Hz
3.0

@Frequency 1.00e+6 Hz
DIN 53 483, IEC-250
Dielectric Strength 27.0 kV/mm
686 kV/in
Breakdown; DIN 53 481, IEC-243, VDE 0303 Part 1
Dielectric Loss Index 0.0060

@Frequency 1.00e+6 Hz
0.0060

@Frequency 1.00e+6 Hz
DIN 53 483, IEC-250
Descriptive Properties Value Comments
Color transparent
Creep Resistance Grade CTI 350
DIN 53 480, IEC-112, VDE 0303 Part 1
Resistance to hot water, suds not resistant