Mechanical Properties Metric English Comments
Tensile Strength 65.0 MPa
9430 psi
ASTM D638
Premix Premi-Glas® 1261-28 VE Glass Reinforced Vinyl Ester TMC
Description: Premi-Glas® 1261-28 VE is a glass reinforced vinyl ester molding compound designed for automotive under the hood applications. Key features and benefits: Excellent thermal stability an..
Tensile Strength 65.0 MPa
9430 psi
ASTM D638
Premix Premi-Glas® 2200-25 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2200-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Tensile Strength 65.0 MPa
9430 psi
ASTM D638
Premix Premi-Glas® 2203-25 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2203-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Tensile Strength 65.0 MPa
9430 psi
ASTM D638
Premix Premi-Glas® 2203-25 CR-SX-HT Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2203-25 CR-SX-HT is a fiberglass reinforced thermoset sheet molding compound for electrical and flame retardant applications.Key features and benefits are:Enhanced product for higher UL..
Tensile Strength 65.0 MPa
9430 psi
ASTM D638
Premix Premi-Glas® 2204-25 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2204-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Tensile Strength 65.0 MPa
9430 psi
ASTM D638
Premix Premi-Glas® 2205-25 CR-SX Fiberglass Reinforced SMC
Description: Premi-Glas® 2205-25 CR-SX is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal ..
Tensile Strength 65.0 MPa
9430 psi
ASTM D638
Premix Premi-Glas® 2207-20 CR-SX Fiberglass Reinforced Thermoset SMC
Premi-Glas® 2207-20 CR-SX is a fiberglass reinforced thermoset sheet molding compound for electrical, flame retardant and HVAC applications.Key features and benefits are:Non-Halogen FR technology f..
Tensile Strength 65.0 MPa
9430 psi
ASTM D638
Premix Premi-Glas® 2243-24 CR-SX Fiberglass Reinforced Thermoset Thick Molding Compound
Premi-Glas® 2243-24 CR-SX is a fiberglass reinforced thermoset thick molding compound for electrical and flame retardant applications.Key features and benefits are:TMC compounding process preserves..
Tensile Strength 65.0 MPa
9430 psi
ASTM D638
Premix Premi-Glas® 3200-25 Fiberglass Reinforced SMC
Description: Premi-Glas® 3200-25 is a fiberglass reinforced thermoset Sheet Molding Compound formulated for excellent electrical properties and fire retardance; it also has very good thermal and di..
Tensile Strength 65.0 MPa
9430 psi
ASTM D638
Kolon KOCETAL® K500 Standard Grade Acetal Resin
General injection molding grade. Easy flow grade for hard-to fill molds and mechanical thin-wall parts.Applications: General injection molding products.Information provided by API-Kolon.
Tensile Strength 65.0 MPa
9430 psi
ASTM D638
Kolon KOCETAL® K700BK Colored Grade Acetal Resin
Colored, low viscosity grade.Applications: Thin products, improved appearance.Information provided by API-Kolon.
Tensile Strength 65.0 MPa
9430 psi
ASTM D638
Kolon KOCETAL® TC701 Mineral Reinforced Acetal Resin
Talc reinforced, improved dimensional stability. Applications: Products for high stiffness, dimensional precision. Information provided by API-Kolon.
Tensile Strength 65.0 MPa
9430 psi
ISO 527
Lucite International Diakon® TD510 Toughened Acrylic Compound
The Diakon® impact PMMA series offer the best combination of impact, chemical and heat resistance and provide rigidity and surface hardness.The grades in the Diakon® series can be processed by..
Tensile Strength 65.0 MPa
9430 psi
DIN 53455
Isoflon POM C Polyacetal C
Good optical propertiesHigh UV resistanceAbsorbs little moistureInformation provided by Isoflon.
Tensile Strength >= 65.0 MPa
>= 9430 psi
GB/T 1040.2-2006
Sichuan Deyang Haton® hc Polyphenylene Sulfide Resin
Fiber gradeInformation provided by Sichuan Deyang Chemical Co., LTD
Tensile Strength 65.0 MPa
9430 psi
50 mm/min; ISO 527-1
Sax Polymers SAXAMID 136F3Q32 Nylon 6, 15% Glass Fiber
SAXAMID 136F3Q32 is a high-impact-modified polyamide 6 injection-molding-grade reinforced with 15% glass fibers with very high impact properties. Beside the high impact strength at low temperatures ..
Tensile Strength 65.0 MPa
9430 psi
dry; ISO 527
Ter Hell Plastic Terez® PA 6 7750 TK Polyamide 6
Description: Medium viscosity, high impact modified standard grade PA 6, with crystallization accelerator and good flowability.Application: For molding parts with high impact stress.Information pr..
Tensile Strength 65.0 MPa
9430 psi
cond.; DIN 53 455
Hippe PA 46 Nylon 46
PA 46 is primarily used in higher temperature ranges where stiffness, creep resistance, continuous heat stability and fatigue strength are required. Therefore PA 46 is suitable for high quality app..
Tensile Strength 65.0 MPa
9430 psi
DIN 53 455
Hippe PC Polycarbonate
Hard, stiff, very good impact properties with a wide range of temperature (to -100°C). High stability of shape under heat. Clear with own slight yellowish color. Low water absorption, weather-re..
Tensile Strength 65.0 MPa
9430 psi
DIN 53 455
Hippe POM Copolymer
Polyacetals are particularly suitable for the manufacture of precision and technical components, bushing, spring elements, housing components, sliding elements, chains, curve discs, bearing, running..
Tensile Strength 65.0 MPa
9430 psi
50 mm/min; ISO 37
BASF Elastollan R 2005/1 20% Glass Filled TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan..
Tensile Strength 65.0 MPa
9430 psi
50 mm/min; ISO 37
BASF Elastollan R 2006 20% Glass Filled TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan..
Tensile Strength 65.0 MPa

@Strain 2.00 %,
Temperature 0.000 °C
9430 psi

@Strain 2.00 %,
Temperature 32.0 °F
50 mm/min; ISO 527-2
BASF Elastollan R 3000 20% Glass Filled TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan..
Tensile Strength 65.0 MPa
9430 psi
50 mm/min; ISO 37
BASF Elastollan R 3001 15% Glass Filled TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan..
Tensile Strength 65.0 MPa
9430 psi
cond.; ISO 527
Azoty Tarnow™ Tarnamid® T-27 GF15 Polyamide 6 - Glass Fiber Reinforced
15% Glass fiber reinforced, medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High..
Tensile Strength 65.0 MPa
9430 psi
50 mm/min; ISO 37
BASF Elastollan R 2000 20% Glass Filled TPUR
Description: Thermoplastic Polyester Polyurethane Elastomers with exceptional properties, very high impact resistance, high modulus with at the same time elasticity, low coefficient of thermal expan..
Tensile Strength 65.02 MPa

@Temperature 23.0 °C,
Time 2.42e+6 sec
9430 psi

@Temperature 73.4 °F,
Time 672 hour
Thirty mil sheet immersion
Lubrizol ESTANE® 58277 Ester Based Thermoplastic Polyurethane
Features: Excellent physical properties, good chemical resistance and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion and Injection and blow molding.Complies with: ..
Tensile Strength 65.02 MPa

@Temperature 23.0 °C,
Time 5.011e+6 sec
9430 psi

@Temperature 73.4 °F,
Time 1392 hour
Thirty mil sheet immersion
Lubrizol ESTANE® 58277 Ester Based Thermoplastic Polyurethane
Features: Excellent physical properties, good chemical resistance and wide processing window for extrusion.Uses: Blown and flat die/cast film extrusion and Injection and blow molding.Complies with: ..