Material Notes:
This product is phenols antioxidant, applicable to the occasion that there are liquor, latex, soliquoid and mixture,especially applicable to polyols and polyurethane.it has excellent effect in anti-burning if it is dipped in polyurethane. The product also can prevent polyols producing Peroxidase in storage process,it also has the anti-fogging function in polyurethane froth Cotton,and has good antioxidant effect in multiplicate polymer. The advised quantities:0.5~1.0%Chemical Name: Benzenepropanoic acid,3,5-bis(1,1-dimethylethyl)-4-hydroxy-C7-C9 branched alkyl estersCAS No. 125643-61-0All information provided by Hongkun Group
Physical Properties Metric English Comments
Density 0.950 - 1.00 g/cc

@Temperature 20.0 °C
0.0343 - 0.0361 lb/in³

@Temperature 68.0 °F
Solubility <= 100 ppm

@Temperature 20.0 °C
<= 100 ppm

@Temperature 68.0 °F
Water
>= 50000 ppm

@Temperature 20.0 °C
>= 50000 ppm

@Temperature 68.0 °F
Esters
<= 100000 ppm

@Temperature 20.0 °C
<= 100000 ppm

@Temperature 68.0 °F
Polyether polyols
>= 500000 ppm

@Temperature 20.0 °C
>= 500000 ppm

@Temperature 68.0 °F
Trichloromethane
>= 500000 ppm

@Temperature 20.0 °C
>= 500000 ppm

@Temperature 68.0 °F
Acetone
>= 500000 ppm

@Temperature 20.0 °C
>= 500000 ppm

@Temperature 68.0 °F
Methyl Alcohol
>= 500000 ppm

@Temperature 20.0 °C
>= 500000 ppm

@Temperature 68.0 °F
Ethyl Acetate
>= 500000 ppm

@Temperature 20.0 °C
>= 500000 ppm

@Temperature 68.0 °F
Dichloromethane
>= 500000 ppm

@Temperature 20.0 °C
>= 500000 ppm

@Temperature 68.0 °F
Benzene
>= 500000 ppm

@Temperature 20.0 °C
>= 500000 ppm

@Temperature 68.0 °F
Polyester polyols
Viscosity Measure 250 - 600 cSt

@Temperature 20.0 °C
250 - 600 cSt

@Temperature 68.0 °F
Thermal Properties Metric English Comments
Melting Point <= 10.0 °C
<= 50.0 °F
Boiling Point >= 200 °C
>= 392 °F
Flash Point >= 152 °C
>= 306 °F
uncork
Optical Properties Metric English Comments
Refractive Index 1.493 - 1.499
1.493 - 1.499
Chemical Properties Metric English Comments
Acid Value <= 0.10
<= 0.10
mg KOH/g
Processing Properties Metric English Comments
Moisture Content <= 0.10 %
<= 0.10 %
Descriptive Properties Value Comments
Appearance clear, colorless or light yellow liquor
Purity (%) >= 98
Users viewing this material also viewed the following: