Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Hoskins Manufacturing Alumel® Thermocouple Wire Type K - Std

Category Metal , Nonferrous Metal , Nickel Alloy
Manufacturer Hoskins Manufacturing
Trade Name Alumel®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hoskins Manufacturing Alumel® Thermocouple Wire Type K - Std.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
All values may vary dependent on specific design and usageAlumel® is a registered trade name of Hoskins Manufacturing.Capabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire.
Physical Properties Metric English Comments
Density 8.61 g/cc
0.311 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength at Break 586 MPa
85000 psi
Annealed
1030 MPa
150000 psi
Stress relieved
1170 MPa
170000 psi
Hard
Thermal Properties Metric English Comments
CTE, linear 12.0 µm/m-°C

@Temperature 20.0 °C
6.67 µin/in-°F

@Temperature 68.0 °F
Specific Heat Capacity 0.523 J/g-°C

@Temperature 20.0 °C
0.125 BTU/lb-°F

@Temperature 68.0 °F
Thermal Conductivity 29.7 W/m-K
206 BTU-in/hr-ft²-°F
Melting Point 1260 °C
2300 °F
Maximum Service Temperature, Air 1260 °C
2300 °F
Operating Temperature
Component Elements Properties Metric English Comments
Aluminum, Al 2.0 %
2.0 %
Manganese, Mn 2.0 %
2.0 %
Nickel, Ni 95 %
95 %
Electrical Properties Metric English Comments
Electrical Resistivity 0.0000294 ohm-cm
0.0000294 ohm-cm
3% tolerance on sizes below 0.02, 5% tolerance on sizes above 0.02
Descriptive Properties Value Comments
Magnetic Strong
Temperature Coefficient of Resistance 0.00188 ohms/ohm-°C
0-100°C
Users viewing this material also viewed the following: