Material Notes:
Approx. H+ equivalent weight 63. Mix Ratio with GY 6010 is 36.Comments/Applications: 4,4'-diaminodiphenyl sulfone (DDS). Solid amine with a melting point of 174 - 178°C. Excellent high temperature and chemical resistance. Adhesives, PWB laminates, prepregs, composites.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 174 - 178 °C
345 - 352 °F
Softening Range
Processing Properties Metric English Comments
Processing Temperature 175 °C
347 °F
Cure Schedule: 4 hrs. at 175°C or 24 hrs at 120°C.
Pot Life 180 min

@Temperature 100 °C
180 min

@Temperature 212 °F