Huntsman HY 360 Polyamide

Category Polymer , Thermoset , Epoxy
Manufacturer Huntsman, former Ciba Specialty Chemicals
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Huntsman HY 360 Polyamide.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Approx. H+ equivalent weight 134. Mix Ratio with GY 6010 is 60.Comments/Applications: Very low viscosity, modified polyamidoamine; compatible with bis F resins. Superior chemical resistance. Ultra high solids/solventless coatings. Maintenance and marine primers.Data provided by Ciba Specialty Chemicals.Ciba Specialty Chemicals has been acquired by Huntsman.
Physical Properties Metric English Comments
Viscosity 300 - 500 cP
300 - 500 cP
Processing Properties Metric English Comments
Pot Life 450 min
450 min