Physical Properties | Metric | English | Comments |
---|---|---|---|
Viscosity | 300 - 500 cP | 300 - 500 cP | |
ND Industries 388 Toughened Instant Superglue Black toughened Cyanoacrylate for metal, rubber, and plastic |
|||
Viscosity | 90 - 500 cP @Temperature 25.0 °C |
90 - 500 cP @Temperature 77.0 °F |
|
Northstar Polymers MNB-013 Isocyanate Prepolymer Information provided by Northstar Polymers. |
|||
Viscosity | 300 - 500 cP @Temperature 25.0 °C |
300 - 500 cP @Temperature 77.0 °F |
Mixed |
Resin Technology Group UV MX-2240 Multi-Functional Hybrid, UV-Curing, Micro-Electronic System Mix ratio 2 to 1 by volume.UV-MX 2240 is a low-viscosity, water-white photo/ chemical cross-linking encapsulant/sealant designed for micro-electronic applications. This two-part, Hybrid UV-epoxy bas.. |
|||
Viscosity | 250 - 500 cP | 250 - 500 cP | |
Huntsman HY 9130 Polyamide Approx. H+ equivalent weight 95. Mix Ratio with GY 6010 is 50.Comments/Applications: Low viscosity polyamidoamine for solvent free systems. Good mechanical properties. Adhesives, sealants, floor.. |
|||
Viscosity | 290 - 500 cP | 290 - 500 cP | |
Huntsman HY 956 Aliphatic Amine Approx. H+ equivalent weight 47. Mix Ratio with GY 6010 is 25.Comments/Applications: Low viscosity liquid amine with low shrinkage, excellent dimensional stability, good electricals. Adhesives, c.. |
|||
Viscosity | 125 - 500 cP @Temperature 25.0 °C |
125 - 500 cP @Temperature 77.0 °F |
|
Lord Adhesives Flocklok® 550P Flock Adhesive LORD Flocklok® 550P adhesive is a single-coat adhesive used to adhere polyester or nylon flock fibers to a variety of uncured and semi-cured elastomers including EPDM, NR, CR and SBR. Flocked sub.. |
|||
Viscosity | 301 - 500 cP | 301 - 500 cP | ASTM D445 |
IRPC Polimaxx Polene PE300N Polypropylene Wax APPLICATIONS: CARRIER FOR PIGMENT CONCENTRATES, LUBRICANT FOR PLASTICS, RUBBER EXTRUSION, HOT MELT ADHESIVE, PAPER COATING |
|||
Viscosity | 250 - 500 cP | 250 - 500 cP | 10% Toluene Solution at 25°C; KM 06 |
Kraton® G1654 E (SEBS) Linear Triblock Copolymer Description: Kraton G1654 E polymer is a clear, linear triblock copolymer based on styrene and ethylene/butylene, S-E/B-S, with bound styrene of 30% mass. It is supplied from Europe in the physical .. |
|||
Viscosity | 400 - 500 cP @Temperature 23.0 °C |
400 - 500 cP @Temperature 73.4 °F |
|
Master Bond EP30 Optically Clear, Low Viscosity Two Component Epoxy Master Bond Polymer System EP30 is a low viscosity, two component epoxy system for high performance bonding, coating, sealing, potting and encapsulation. It readily cures at room temperature or more.. |
|||
Viscosity | 280 - 500 cP | 280 - 500 cP | Part B |
Master Bond EP30ANHT Two Part, Electrically Isolating Epoxy Adhesive Description: Master Bond Polymer System EP30ANHT is a two part epoxy system with terrific thermal conductivity, while maintaining electrical insulation. One noteworthy property is its wide service t.. |
|||
Viscosity | 280 - 500 cP | 280 - 500 cP | Part B |
Master Bond EP30AOHT Dimensionally Stable, Two Component Epoxy Description: Master Bond Polymer System EP30AOHT is a two component epoxy resin system for high performance bonding, potting, sealing and coating, formulated to cure at room temperature or more rapi.. |
|||
Viscosity | 250 - 500 cP | 250 - 500 cP | Part B |
Master Bond EP30HT-LO NASA Low Outgassing, Optically Clear Coating Description: Master Bond EP30HT-LO is a moderate viscosity, two component epoxy adhesive formulated to cure at room temperature or more rapidly at elevated temperatures, with a four to one mix ratio.. |
|||
Viscosity | 400 - 500 cP | 400 - 500 cP | mixed |
Master Bond EP37-3FLSP Optically Clear Epoxy Has Low Exotherm Description: Master Bond EP37-3FLSP is a very flexible, low viscosity, optically clear two component epoxy resin system designed for high performance bonding, coating and casting applications. It fe.. |
|||
Viscosity | 280 - 500 cP | 280 - 500 cP | Part B |
Master Bond EP30LV-1 Ultra Low Viscosity, Two Part Epoxy System Description: Master Bond Polymer System EP30LV-1 is an ultra low viscosity, two component epoxy system for high performance bonding, coating, sealing, potting and encapsulation. It readily cures at .. |
|||
Viscosity | 200 - 500 cP | 200 - 500 cP | NOV QC 020 |
Lubrizol ESTANE® 5719 Ester Based Thermoplastic Polyurethane (European Grade) Description: Estane® thermoplastic polyurethanes (TPUs) include elastomeric materials that bridge the gap between flexible rubber and rigid plastics. These materials offer toughness and durability .. |
|||
Viscosity | 300 - 500 cP | 300 - 500 cP | |
C.O.I.M. FILCO® 300 Non Ionic Epoxy-Polyester Aqueous Emulsion for Glass Fiber Sizing Description: Non Ionic Epoxy-Polyester Aqueous Emulsion for Glass Fiber SizingGeneral Information: COIM has developed a range of polyesters for the treatment of glass fiber. These polyesters come in.. |
|||
Viscosity | 350 - 500 cP @Temperature 35.0 °C |
350 - 500 cP @Temperature 95.0 °F |
Dynamic viscosity |
C.O.I.M. PLAXTER® P 90 Polymeric Plasticizer Description: Formulated with PVC, it is used in the field of synthetic leathers.Information provided by P.A.T. Products, Inc. |
|||
Viscosity | 200 - 500 cP | 200 - 500 cP | |
Aremco Corr-Paint™ CP3015-SS High Temperature Protective Coating Inorganic, Mixed Oxides Filled These inorganic-ceramic, aqueous-based coatings provide outstanding resistance to thermal shock, oxidation and chemical corrosion in 1500°F. Stainless steel filled, inorganic coating to 1400°F. |
|||
Viscosity | 250 - 500 cP | 250 - 500 cP | |
Aremco Corr-Paint™ CP4000-S1 High Temperature Protective Coating, Silicone |
|||
Viscosity | 250 - 500 cP | 250 - 500 cP | |
Aremco Corr-Paint™ CP4010-S1 High Temperature Protective Coating, Silicone |
|||
Viscosity | 300 - 500 cP | 300 - 500 cP | |
Aremco Corr-Paint™ CP4080-S High Temperature Protective Coating, Silicone-Polyester |
|||
Viscosity | 300 - 500 cP | 300 - 500 cP | |
Aremco Corr-Paint™ CP4080-S1 High Temperature Protective Coating, Silicone |
|||
Viscosity | 300 - 500 cP | 300 - 500 cP | |
Aremco Corr-Paint™ CP4090-S1 High Temperature Protective Coating, Silicone |
|||
Viscosity | 350 - 500 cP | 350 - 500 cP | blended |
Abatron AboCast 7802-1/AboCure 7804-3 (80 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-3 a clear, slightly accelerated converter for lower rigidity. It has an HDT of 60°C, v.. |
|||
Viscosity | 350 - 500 cP | 350 - 500 cP | blended |
Abatron AboCast 7802-1/AboCure 7804-4 (80 pbw) Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 7804-4 a clear, more accelerated converter for lower rigidity. It has an HDT of 60°C, varia.. |
|||
Viscosity | 300 - 500 cP | 300 - 500 cP | |
Aremco Corr-Paint™ CP4050-S1 High Temperature Protective Coating, Silicone |
|||
Viscosity | 300 - 500 cP | 300 - 500 cP | blended |
Abatron AboCast 7802-1/AboCure 50-12 Epoxy AboCast 7802-1 is a clear resin with low viscosity (600-800 cps.) and a weight of 9.1 lbs/gallon. AboCure 50-12 is a clear converter for high rigidity, chemical, and temperature resistance (HDT: 101.. |
|||
Viscosity | 30.0 - 500 cP @Temperature 230 - 270 °C |
30.0 - 500 cP @Temperature 446 - 518 °F |
Average value: 188 cP Grade Count:2 |
Overview of materials for Nylon 6, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Viscosity | 30.0 - 500 cP @Shear Rate 100 - 10000 1/s |
30.0 - 500 cP @Shear Rate 100 - 10000 1/s |
Average value: 188 cP Grade Count:2 |
Overview of materials for Nylon 6, 30% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Glass Fiber Filled". Specific grades with glass content between 25% and 34% are included. E.. |
|||
Viscosity | 200 - 500 cP | 200 - 500 cP | |
Epoxyset Epoxibond EB-177 Unfilled Epoxy Adhesive A two-component, unfilled, high temperature epoxy adhesive used for bonding and small potting applications in the medical, electronics, and aerospace industries.Information provided by Epoxyset Inc... |