Hyosung Topilene B301 PP

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Hyosung Co.
Trade Name Topilene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hyosung Topilene B301 PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
B301 HomopolymerApplications:Thermoforming sheetsCharacteristics:High melt tensionDimensional stabilityGood optical propertyInformation provided by Hyosung Corporation
Physical Properties Metric English Comments
Melt Flow 1.4 g/10 min
1.4 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95
95
ASTM D785
Tensile Strength, Yield 39.2 MPa
5690 psi
ASTM D638
Flexural Modulus 1.81 GPa
263 ksi
ASTM D790
Izod Impact, Unnotched 0.490 J/cm
0.918 ft-lb/in
ASTM D256