Hyosung Topilene J640 PP

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Hyosung Co.
Trade Name Topilene
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hyosung Topilene J640 PP.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
J640 Injection Impact CopolymerApplications:General purposeBattery caseElectric applianceCharacteristics:Medium ImpactFlowabilityInformation provided by Hyosung Corporation
Physical Properties Metric English Comments
Melt Flow 10 g/10 min
10 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80
80
ASTM D785
Tensile Strength, Yield 27.5 MPa
3980 psi
ASTM D638
Elongation at Break 400 %
400 %
ASTM D638
Flexural Modulus 1.18 GPa
171 ksi
ASTM D790
Izod Impact, Unnotched 0.981 J/cm
1.84 ft-lb/in
ASTM D256
0.490 J/cm

@Temperature -10.0 °C
0.918 ft-lb/in

@Temperature 14.0 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
ASTM D648
Vicat Softening Point 150 °C
302 °F
ASTM D1525
Flammability, UL94 HB
HB