Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.18 GPa | 171 ksi | at 1% Secant; ASTM D790 |
NOVA Chemicals Novapol® HB-L354-A HDPE Blow Molding Resin Good balance of physical and molding properties-high toughness, Excellent processability on high-speed, multiple-head blow molding lines, UL-94HB listedApplications: Household chemical bottles, Indu.. |
|||
Flexural Modulus | 1.18 GPa | 171 ksi | ASTM D790 |
PolyMirae Moplen EP340G Sheet and Thermoforming Grade Polypropylene Moplen RP340G is the polypropylene random copolymer polymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP340G is a random copolymer particularly suitable for.. |
|||
Flexural Modulus | 1.18 GPa | 171 ksi | 3 pt. secant. ASTM D790 |
Chevron Phillips HiD® 9410 HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Wide Range of Processing Conditions, Good Parison Uniformity, Good TrimabilityApplications:Phar.. |
|||
Flexural Modulus | 1.18 GPa | 171 ksi | 3 pt. secant. ASTM D790 |
Chevron Phillips HiD® 9412/HiD® 9413 with Antistat HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding, Injection Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flo.. |
|||
Flexural Modulus | 1.18 GPa | 171 ksi | 3 pt. secant. ASTM D790 |
Chevron Phillips HiD® 99413F with Food Grade Antistat HDPE Blow Molding Resin
(discontinued **) Resin Type: Linear Copolymer; Blow Molding, Injection Blow Molding ResinCharacteristics: Medium Molecular Weight Distribution, Reduced Yellow Potential, Wide Range of Processing Conditions, Good Flo.. |
|||
Flexural Modulus | 1.18 - 13.8 GPa | 171 - 2000 ksi | Average value: 9.49 GPa Grade Count:167 |
Overview of materials for Nylon 6, 40% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Glass Fiber Filled". Specific grades with glass content between 35% and 44% are included. E.. |
|||
Flexural Modulus | 1.18 GPa | 171 ksi | ASTM D790 |
Hyosung Topilene B240P PP B240P Extrusion Impact CopolymerApplications:Pipe (drain, etc…)Characteristics:Pressure resistanceHigh impactLong-term heat stabilityInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.18 GPa | 171 ksi | ASTM D790 |
Hyosung Topilene J440 PP J440 Injection Impact CopolymerApplications:CrateContainerBatter caseCharacteristics:High ImpactInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.18 GPa | 171 ksi | ASTM D790 |
Hyosung Topilene J640 PP J640 Injection Impact CopolymerApplications:General purposeBattery caseElectric applianceCharacteristics:Medium ImpactFlowabilityInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.18 GPa | 171 ksi | ASTM D790 |
Hyosung Topilene J640U PP J640U Injection Impact CopolymerApplications:General purposeBattery caseElectric applianceCharacteristics:Medium ImpactFlowabilityWeatherabilityInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.18 GPa | 171 ksi | ASTM D790 |
Hyosung Topilene R301 PP R301 Extrusion Random CopolymerApplications:Extrusion blow moldingThermoforming sheetCharacteristics:TransparencyStiffnessStretchabilityInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.18 GPa | 171 ksi | ASTM D790 |
Hyosung Topilene R401 PP R401 Extrusion Random CopolymerApplications:Extrusion blow moldingStationary sheetCharacteristics:TransparencyStiffnessInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.18 GPa | 171 ksi | ASTM D790 |
Hyosung Topilene R801 PP R801 Injection Random CopolymerApplications:High transparent productLarge articlesCharacteristics:High transparencyStiffnessInformation provided by Hyosung Corporation |
|||
Flexural Modulus | 1.18 GPa @Thickness 3.20 mm |
171 ksi @Thickness 0.126 in |
2.8mm/min; ASTM D790 |
LG Chemical LUMID GP1300AP PA6, Plasticized Feature: Injection Molding, PA6, PlasticizedApplication: Automotive PartsInformation provided by LG Chemical |
|||
Flexural Modulus | 1.18 GPa @Thickness 6.40 mm |
171 ksi @Thickness 0.252 in |
30mm/min; ASTM D790 |
LG Chemical LUPOL EI5002 PP Description: Injection Molding, PP, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 9002-88-4Information provided by LG Chemical |
|||
Flexural Modulus | 1.18 GPa | 171 ksi | ASTM D790 |
LG Chemical SEETEC PB270 HDPE Features: This high molecular weight, hexane copolymer is tailored for light-weight blow-molded containers that require: Good stiffness and Excellent processabilityAdditives: Anti-OxidantsApplicatio.. |
|||
Flexural Modulus | 1.18 GPa | 171 ksi | ASTM D790 |
LG Chemical SEETEC PF150 HDPE Features: Characteristics: Good impact & tear strength, High speed & superior heat sealing propertiesAdditives: Anti-oxidants, LubricantsApplication: Shopping bags, Thin films, Trash bags, Multiwall.. |
|||
Flexural Modulus | 1.18 GPa | 171 ksi | ASTM D760 |
LG Chemical SEETEC R1610 Polypropylene Random Copolymer Features: SEETEC R1610 is a highly transparent ethylene-propylene random copolymer for injection molding applications. SEETEC R1610 exhibits an excellent transparency and a good impact strength. SEE.. |
|||
Flexural Modulus | 1.18 GPa | 171 ksi | ASTM D790B |
Lotte Chemical Titan TITANPRO® EPC40R Polypropylene impact copolymer The base resin meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520(a)(3)(i) and (c)3.1a. The adjuvants meet their respective FDA regulations and 21 CFR 1.. |
|||
Flexural Modulus | 1.18 GPa | 171 ksi | ASTM D790 |
LG Chemical LUPOL TE-5104K Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Modulus LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Flexural Modulus | 1.18 GPa | 171 ksi | ASTM D790 |
SCG Chemicals EL-Leneâ„¢ H5840B High Density Polyethylene Blow Molding Key Characteristics:Excellent environmental stress cracking resistance (ESCR)Excellent appearanceOdorlessSafe for food contactGood printabilityRecommended Applications: Bottles for food, juice, sof.. |
|||
Flexural Modulus | 1.18 GPa | 171 ksi | ASTM D790 |
SCG Chemicals EL-Proâ„¢ P640J Polypropylene Injection Molding Key Characteristics:Good flowabilityHigh stiffnessHigh impact strengthRecommended Applications:High impact electrical appliance parts, automotive and motorcycle parts such as fan stand, washing tubI.. |
|||
Flexural Modulus | 1.18 GPa | 171 ksi | ASTM D790 |
SCG Chemicals EL-Proâ„¢ P750J Polypropylene Injection Molding Key Characteristics:Excellent clarityHigh productivityGood processability and stiffnessHigh glossOdorlessSafe for food contactRecommended Applications:Food container, utensilMedical parts such as sy.. |
|||
Flexural Modulus | 1.18 GPa | 171 ksi | ASTM D790 |
Total PPC 4524WZ Polypropylene, Impact Copolymer TOTAL Petrochemicals Polypropylene 4524WZ is a nucleated high impact copolymer with a Melt Flow index of 7 g/10 min.TOTAL Polypropylene 4524WZ is characterized by significantly improved impact resis.. |
|||
Flexural Modulus | 1.18 GPa | 171 ksi | 0.039 in/min; ISO 178 |
ExxonMobil Exxtral™ BMU130A Performance Polyolefin Product Description: Polyolefin injection molding compound with a good balance of stiffness, flow, and excellent processability for automotive bumper fascia and exterior trim applicationsAvailabilit.. |
|||
Flexural Modulus | 1.18 GPa | 171 ksi | ASTM D790 |
Equate EMDA-6147 HDPE Blow Molding Resin EMDA-6147 is a high density polyethylene copolymer resin designed for blow molding of large size containers. Its high molecular weight and broad molecular weight distribution with a balanced density.. |
|||
Flexural Modulus | 1.18 GPa | 171 ksi | ASTM D790 |
Equate EPDA-5040 HDPE Non-Pressure Gravity Pipe Resin EPDA-5040 is a high molecular weight high density polyethylene copolymer resin designed for non-pressure gravity pipe applications. It has a good balance of flexibility, ductility, stiffness and tou.. |
|||
Flexural Modulus | 1.18 GPa | 171 ksi | Conditioned 15 days at 23°C - 50% RH; ISO 178 |
Arkema Group Rilsamid® PA 12 AESNO MED Nylon 12 Rilsamid® AESNO MED is a rigid polyamide 12 with high viscosity designed for tube extrusion. This grade dedicated to extrusion offers the highest quality and it is specifically designed to meet the.. |
|||
Flexural Modulus | 1.18 GPa | 171 ksi | ASTM-D-790 |
BCC Products LIK-WOOD BC 8007 Urethane Casting Lik-Wood is a low viscosity, quick setting, easy to use casting material. A model or tool cast from Lik-Wood will weigh 60% less than other filled urethane systems. Within 30 minutes after mixing an.. |
|||
Flexural Modulus | 1.18 GPa | 171 ksi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON MS000IL PP LNP* STAT-KON* MS000IL is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: High Impact, Low Extractible, Electrically Conductive, food c.. |