Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

I. Stern 1320NA Prime Homopolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer I. Stern & Company
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF I. Stern 1320NA Prime Homopolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Features:Good flow characteristicsAntistat propertiesLow odorApplicationsThin wall packagingSmall appliancesAutomotiveInformation provided by I. Stern & Co. Inc.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D1505
Melt Flow 21 g/10 min
21 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 37.8 MPa
5480 psi
51 mm/min; ASTM D638
Elongation at Yield 13 %
13 %
51 mm/min; ASTM D638
Flexural Modulus 1.86 GPa
270 ksi
1% Secant, 1.27 mm/min; ASTM D790A
Izod Impact, Notched 0.267 J/cm
0.500 ft-lb/in
ASTM D256
Users viewing this material also viewed the following: