ICO Polymers ICORENEâ„¢ 115-1037 LMDPE Rotational Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Linear Medium Density Polyethylene (LMDPE), Rotational Molded
Manufacturer ICO Polymers (A Schulman Inc.)
Trade Name ICORENE™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ICO Polymers ICORENEâ„¢ 115-1037 LMDPE Rotational Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: ICORENE 115-1037 polyethylene developed for use in rotational molding. It is an easy processing material with good surface gloss, scratch resistance and generally balanced physical properties. This product is enhanced by ICOPower and OptiFlo. The base resin is FDA approved and is fully stabilized to UV8 level. Key Characteristics: easy processing, good rigidity, good scratch resistance. Applications: This ICORENE® grade is particularly suitable for use in playground applications. Information provided by ICO Polymers.A Schulman acquired ICO, Inc. in 2010.
Physical Properties Metric English Comments
Density 0.940 g/cc
0.0340 lb/in³
ASTM D1505
Melt Index of Compound 5.1 g/10 min

@Load 2.16 kg,
Temperature 190 °C
5.1 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 61
61
ASTM D2240
Tensile Strength, Yield 20.30 MPa
2944 psi
2"/min; ASTM D638
Elongation at Break 360 %
360 %
2"/min; ASTM D638
Flexural Modulus 0.74994 GPa
108.77 ksi
ASTM D790
Impact 22.5

@Temperature -20.0 °C
22.5

@Temperature -4.00 °F
J/mm, instrumented impact, rotomolded test sample; ICO R&D1.14