Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

IDI Composites 46-3 Thermoset Polyester, Molding

Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer IDI Composites
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IDI Composites 46-3 Thermoset Polyester, Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Superior electrical performance with low pressure molding for V-O flammability in encapsulation applications.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.80 g/cc
0.0650 lb/in³
Water Absorption 0.15 %
0.15 %
in 24 hours; ASTM D570
Linear Mold Shrinkage 0.00040 - 0.0020 cm/cm
0.00040 - 0.0020 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 20 - 30
20 - 30
ASTM D2583
Tensile Strength, Ultimate 24.0 MPa
3480 psi
ASTM D638
Flexural Strength 62.0 MPa
8990 psi
ASTM D790
Compressive Strength 90.0 MPa
13100 psi
ASTM D695
Izod Impact, Notched 1.10 J/cm
2.06 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 204 °C
>= 399 °F
ASTM D648
Flammability, UL94 V-0

@Thickness 3.20 mm
V-0

@Thickness 0.126 in
Electrical Properties Metric English Comments
Arc Resistance >= 180 sec
>= 180 sec
ASTM D495
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved