Material Notes:
Premium appearance grade materials in a range of strengths for cookware and appliance applications.Data provided by the manufacturer.
Physical Properties Metric English Comments
Density 1.90 g/cc
0.0686 lb/in³
Water Absorption 0.060 %
0.060 %
in 24 hours; ASTM D570
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Barcol 30 - 40
30 - 40
ASTM D2583
Tensile Strength, Ultimate 59.0 MPa
8560 psi
ASTM D638
Flexural Strength 124 MPa
18000 psi
ASTM D790
Compressive Strength 172 MPa
24900 psi
ASTM D695
Izod Impact, Notched 4.40 J/cm
8.24 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 260 °C
500 °F
ASTM D648
Flammability, UL94 HB

@Thickness 3.20 mm
HB

@Thickness 0.126 in
Electrical Properties Metric English Comments
Dielectric Strength 11.8 kV/mm
300 kV/in
ASTM D149