IRPC Polimaxx Polene 1202J Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer IRPC Polimaxx
Trade Name Polene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IRPC Polimaxx Polene 1202J Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
CHARACTERISTICS: GOOD STIFFNESS, GOOD EXTRUDABILITY, HIGH IMPACTAPPLICATIONS: MONOFILAMENT/YARN/SHEET EXTRUSION AND INJECTION MOLDING COARSE TEXTILE FOR JUMBO BAGS, ROPES, STRAWS, SHEETS, INDUSTRIAL CONTAINERS, STRETCH TAPE, CLOSURES
Physical Properties Metric English Comments
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 107
107
ASTM D785
Tensile Strength, Yield 37.0 MPa
5370 psi
ASTM D638
Elongation at Yield 27.5 %
27.5 %
ASTM D638
Flexural Modulus 1.60 GPa
232 ksi
1% Secant; ASTM D790
Charpy Impact, Notched 0.500 J/cm²

@Temperature 23.0 °C
2.38 ft-lb/in²

@Temperature 73.4 °F
DIN 53453
Thermal Properties Metric English Comments
Heat Distortion Temperature 110 °C
230 °F
ASTM D648
Processing Properties Metric English Comments
Processing Temperature 200 - 280 °C
392 - 536 °F