IRPC Polimaxx Polene PE100N Polypropylene Wax

Category Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer IRPC Polimaxx
Trade Name Polene
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF IRPC Polimaxx Polene PE100N Polypropylene Wax.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
APPLICATIONS: CARRIER FOR PIGMENT CONCENTRATES, LUBRICANT FOR PLASTICS, RUBBER EXTRUSION, HOT MELT ADHESIVE, PAPER COATING
Physical Properties Metric English Comments
Density 0.900 - 0.930 g/cc
0.0325 - 0.0336 lb/in³
TPI Method
Viscosity 1.0 - 30 cP
1.0 - 30 cP
ASTM D445
Mechanical Properties Metric English Comments
Penetration P(0), 1/10 mm 5.0 - 25

@Temperature 25.0 °C
5.0 - 25

@Temperature 77.0 °F
ASTM D1321
Thermal Properties Metric English Comments
Melting Point 108 - 124 °C
226 - 255 °F
ASTM D127
Descriptive Properties Value Comments
Color Pale-White
Product Form Flake