Thermal Properties | Metric | English | Comments |
---|---|---|---|
Melting Point | 108 - 124 °C | 226 - 255 °F | ASTM D127 |
IRPC Polimaxx Polene PE100N Polypropylene Wax APPLICATIONS: CARRIER FOR PIGMENT CONCENTRATES, LUBRICANT FOR PLASTICS, RUBBER EXTRUSION, HOT MELT ADHESIVE, PAPER COATING |
|||
Melting Point | 108 - 124 °C | 226 - 255 °F | ASTM D127 |
IRPC Polimaxx Polene PE200N Polypropylene Wax APPLICATIONS: CARRIER FOR PIGMENT CONCENTRATES, LUBRICANT FOR PLASTICS, RUBBER EXTRUSION, HOT MELT ADHESIVE, PAPER COATING |
|||
Melting Point | 108 - 124 °C | 226 - 255 °F | ASTM D127 |
IRPC Polimaxx Polene PE220NSC Polypropylene Wax APPLICATIONS: CARRIER FOR PIGMENT CONCENTRATES, LUBRICANT FOR PLASTICS, RUBBER EXTRUSION, HOT MELT ADHESIVE, PAPER COATING |
|||
Melting Point | 108 - 124 °C | 226 - 255 °F | ASTM D127 |
IRPC Polimaxx Polene PE250N Polypropylene Wax APPLICATIONS: CARRIER FOR PIGMENT CONCENTRATES, LUBRICANT FOR PLASTICS, RUBBER EXTRUSION, HOT MELT ADHESIVE, PAPER COATING |
|||
Melting Point | 108 - 124 °C | 226 - 255 °F | ASTM D127 |
IRPC Polimaxx Polene PE300N Polypropylene Wax APPLICATIONS: CARRIER FOR PIGMENT CONCENTRATES, LUBRICANT FOR PLASTICS, RUBBER EXTRUSION, HOT MELT ADHESIVE, PAPER COATING |
|||
Melting Point | 112 - 124 °C | 234 - 255 °F | Average value: 121 °C Grade Count:16 |
Overview of materials for Linear Low Density Polyethylene (LLDPE), Compounding Resin This property data is a summary of similar materials in the MatWeb database for the category "Linear Low Density Polyethylene (LLDPE), Compounding Resin". Each property range of values reported is m.. |