Indium Corp. Indalloy 125 Tin-Lead Solder Alloy

Category Metal , Nonferrous Metal , Lead Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 125 Tin-Lead Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 9.07 g/cc
0.328 lb/in³
Thermal Properties Metric English Comments
Melting Point 183 - 227 °C
361 - 441 °F
Solidus 183 °C
361 °F
Liquidus 227 °C
441 °F
Component Elements Properties Metric English Comments
Lead, Pb 55 %
55 %
Tin, Sn 45 %
45 %