Thermal Properties | Metric | English | Comments |
---|---|---|---|
Solidus | 183 °C | 361 °F | |
Indium Corp. Indalloy 113 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 183 °C | 361 °F | |
Indium Corp. Indalloy 118 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 183 °C | 361 °F | |
Indium Corp. Indalloy 141 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 183 °C | 361 °F | |
Indium Corp. Indalloy 145 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 183 °C | 361 °F | |
Indium Corp. Indalloy 149 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 183 °C | 361 °F | |
Indium Corp. Indalloy 153 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 183 °C | 361 °F | |
Indium Corp. Indalloy® 106 (Sn63) Sn-Pb Solder Alloy Standard eutectic tin-lead solder with wide application. Not recommended against silver and/or gold.Information provided by the manufacturer, Indium Corporation. |
|||
Solidus | 183 °C | 361 °F | |
Johnson Matthey JM4060 Soft Solder/Flux General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi.. |
|||
Solidus | 183 °C | 361 °F | Melting Point |
Lucas-Milhaupt 63 Sn-37 Pb Tin/ Silver Solder Characteristics:Although widely used in electronics for both manual and automatic soldering applications, it is also used in general purpose applications where fast alloy flow is desired. This allo.. |
|||
Solidus | 183 °C | 361 °F | |
Indium Corp. Indalloy 108 Tin-Lead Solder Alloy Good pre-tinning alloyInformation Provided by Indium Corporation |
|||
Solidus | 183 °C | 361 °F | |
Indium Corp. Indalloy 109 Tin-Lead Solder Alloy Good electrical grade solderInformation Provided by Indium Corporation |
|||
Solidus | 183 °C | 361 °F | |
Indium Corp. Indalloy 110 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 183 °C | 361 °F | |
Indium Corp. Indalloy 114 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 183 °C | 361 °F | |
Indium Corp. Indalloy 116 Tin-Lead Solder Alloy General purpose solderInformation Provided by Indium Corporation |
|||
Solidus | 183 °C | 361 °F | |
Indium Corp. Indalloy 119 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 183 °C | 361 °F | |
Indium Corp. Indalloy 120 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 183 °C | 361 °F | |
Indium Corp. Indalloy 122 Tin-Lead Solder Alloy Information Provided by Indium Corporation |
|||
Solidus | 183 °C | 361 °F | |
Williams Advanced Alloys WS183 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Solidus | 183 °C | 361 °F | |
Williams Advanced Alloys WS186 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Solidus | 183 °C | 361 °F | |
Williams Advanced Alloys WS188 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Solidus | 183 °C | 361 °F | |
Williams Advanced Alloys WS199 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Solidus | 183 °C | 361 °F | |
Williams Advanced Alloys WS200 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Solidus | 183 °C | 361 °F | |
Williams Advanced Alloys WS205 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Solidus | 183 °C | 361 °F | |
Williams Advanced Alloys WS213 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Solidus | 183 °C | 361 °F | |
Williams Advanced Alloys WS238 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Solidus | 183 °C | 361 °F | |
Williams Advanced Alloys WS257 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Solidus | 183 °C | 361 °F | |
Williams Advanced Alloys WS280 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Solidus | 183 °C | 361 °F | |
Williams Advanced Alloys WS288 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Solidus | 183 °C | 361 °F | |
AIM 63Sn/Pb37 Solder for Photonic Packaging Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials. |
|||
Solidus | 183 °C | 361 °F | |
Johnson Matthey JM6040 Soft Solder/Flux General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materi.. |