Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 8.86 g/cc
0.320 lb/in³
Thermal Properties Metric English Comments
Melting Point 179 - 260 °C
354 - 500 °F
Solidus 179 °C
354 °F
Liquidus 260 °C
500 °F
Component Elements Properties Metric English Comments
Lead, Pb 47 %
47 %
Silver, Ag 3.0 %
3.0 %
Tin, Sn 50 %
50 %