Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Solidus = 354 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Solidus 179 °C
354 °F
Indium Corp. Indalloy 127 Tin-Lead Solder Alloy
Information Provided by Indium Corporation
Solidus 179 °C
354 °F
Indium Corp. Indalloy 142 Tin-Lead Solder Alloy
Information Provided by Indium Corporation
Solidus 179 °C
354 °F
Indium Corp. Indalloy 154 Tin-Lead Solder Alloy
Information Provided by Indium Corporation
Solidus 179 °C
354 °F
Indium Corp. Indalloy 210 Tin-Lead Solder Alloy
Information Provided by Indium Corporation
Solidus 179 °C
354 °F
Indium Corp. Indalloy® Sn62 Sn-Pb-Ag Solder Alloy
Good general purpose solder. Can be used on silver bearing surfaces to reduce scavenging.Information provided by the manufacturer, Indium Corporation.
Solidus 179 °C
354 °F
Indium Corp. Indalloy 104 Tin-Lead Solder Alloy
Widely used electronic solder. Good for silver metallization. Has improved strength and fatigue propertiesInformation Provided by Indium Corporation
Solidus 179 °C
354 °F
Indium Corp. Indalloy 137 Tin-Lead Solder Alloy
Information Provided by Indium Corporation
Solidus 179 °C
354 °F
Williams Advanced Alloys WS179 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Solidus 179 °C
354 °F
AIM 62Sn/Pb36/Ag2 Solder for Photonic Packaging
Uses include:Fiber to Ferrule SolderingLaser Die AttachHermetic Packaging & SealingWetting & Sealing Laser OpticsThermal ManagementInformation provided by AIM Specialty Materials.