Indium Corp. Indalloy 219 Ag-Au-Zn-Cd Solder Alloy

Category Metal , Nonferrous Metal , Precious Metal , Silver Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 219 Ag-Au-Zn-Cd Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 8.88 g/cc
0.321 lb/in³
Thermal Properties Metric English Comments
Melting Point 605 - 700 °C
1120 - 1290 °F
Solidus 605 °C
1120 °F
Liquidus 700 °C
1290 °F
Component Elements Properties Metric English Comments
Cadmium, Cd 18 %
18 %
Copper, Cu 26 %
26 %
Silver, Ag 35 %
35 %
Zinc, Zn 21 %
21 %