Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 8.88 g/cc | 0.321 lb/in³ | |
Materion Brush 1915â„¢ Hard Temper Wire, 0.050" - 0.375" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Density | 8.88 g/cc | 0.321 lb/in³ | |
Materion Brush 1915â„¢ Hard Temper Rod, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Density | 8.88 g/cc | 0.321 lb/in³ | |
Materion Brush 1915™ Heat Treated Temper Rod, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe.. |
|||
Density | 8.88 g/cc | 0.321 lb/in³ | |
Materion Brush 1915™ Heat Treated Temper Wire, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Special Metals FERRY® Alloy A copper-nickel alloy used mainly for its electrical properties. It has medium-range electrical resistivity and a very low temperature coefficient of resistance (TCR). The low TCR makes the alloy .. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Special Metals INCONEL® C276 Nickel Superalloy Plate Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed plate. Other property values are typical of INCO® C276.Data provided by the manufacturer, Specia.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Special Metals INCONEL® C276 Nickel Superalloy Sheet Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed sheet. Other property values are typical of INCO® C276.Data provided by the manufacturer, Specia.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 24% Cold Work Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed + 24% cold worked tubing. Other property values are typical of INCO® C276.Data provided by the m.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 27% Cold Work Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed + 27% cold worked tubing. Other property values are typical of INCO® C276.Data provided by the m.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Special Metals INCONEL® C276 Nickel Superalloy Tubing, 30% Cold Work Tensile strength (ultimate and yield) and elongation values reported here are typical for annealed + 30% cold worked tubing. Other property values are typical of INCO® C276.Data provided by the m.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Special Metals Nickel 200 Commercially pure (99.6%) wrought nickel with good mechanical properties and resistance to a range of corrosive media. Good thermal, electrical, and magnetostrictive properties. Ferromagnetic. Us.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Special Metals Nickel 201 Commercially pure (99.6%) wrought nickel essentially the same as Nickel 200 but with a lower carbon content to prevent embrittlement by intergranular carbon at temperatures over 600°F (315°C)... |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Special Metals Nickel 205 Wrought nickel similar to Nickel 200 but with compositional adjustments to enhance performance in electrical and electronic applications. Ferromagnetic. Used for the anodes and grids of electronic.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Special Metals Nickel 270 A high-purity grade of nickel made by powder metallurgy. It has a low base hardness and high ductility. Its extreme purity is useful for components of hydrogen thyratrons. It is also used for ele.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | As Annealed |
Eagle Brass 200/201 Nickel Alloy, 1/2 Hardened Nickel 200/201 has properties that are useful in industries such as chemical processing and electronics. Nickel is resistant to various reducing chemicals and alkaline materials. Compared with nick.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | As Annealed |
Eagle Brass 200/201 Nickel Alloy, 1/8 Hardened Nickel 200/201 has properties that are useful in industries such as chemical processing and electronics. Nickel is resistant to various reducing chemicals and alkaline materials. Compared with nick.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | As Annealed |
Eagle Brass 200/201 Nickel Alloy, Annealed Nickel 200/201 has properties that are useful in industries such as chemical processing and electronics. Nickel is resistant to various reducing chemicals and alkaline materials. Compared with nick.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | Annealed |
Eagle Brass 725 Copper Nickel Tin, 1/2 Hard Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | Annealed |
Eagle Brass 725 Copper Nickel Tin, 1/4 Hard Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | Annealed |
Eagle Brass 725 Copper Nickel Tin, Annealed Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | Annealed |
Eagle Brass 725 Copper Nickel Tin, Hard Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | Annealed |
Eagle Brass 725 Copper Nickel Tin, Spring Alloy C725 is a moderate strength, low conductivity alloy with excellent bare solderability and corrosion resistance. Applications include electronic parts, springs, connectors and wire wrap termina.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Cadi 182 Copper Alloy Chromium copper is the primary copper alloy used for resistance spot and seam welding. This alloy achieves good hardness and electrical conductivity through a combination of heat treatment and cold .. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
California Fine Wire Nickel 272 Super Alloy All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
California Fine Wire Nickel Alloy 30 Copper Nickel Resistance Wire All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
California Fine Wire Nickel Alloy 99 All values may vary dependent on specific design and usageCapabilities: WireRibbonSquareInsulatedPlatedInformation provided by California Fine Wire. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Carlson C 200 Commercially Pure Nickel General DescriptionCarlson Alloy C 200 is commercially pure nickel, combining good mechanical properties with excellent resistance to many corrosive environments. This alloy retains its strength at.. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Carlson GOC 276 Nickel-Molybdenum-Chromium General DescriptionCarlson Alloy GOC 276 is a nickel-molybdenum-chromium alloy exhibiting outstanding corrosion resistance over a wide range of service environments. This alloy is generally use in .. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Alloy Wire International RW 45 Ni-Cu Resistance Wire Used in thermocouples, power resistors, shunts, and wire wound precision restors up to 750°F (400°C)Information provided by Alloywire International. |
|||
Density | 8.89 g/cc | 0.321 lb/in³ | |
Carlson C 201 Commercially Pure Nickel General DescriptionCarlson Alloy C 200 is commercially pure nickel, combining good mechanical properties with excellent resistance to many corrosive environments. This alloy retains its strength at.. |