Material Notes:
WF-9940 is a highly active no-clean wave solder flux designed for use with through-hole and mixed-technology assemblies. It performs well with both Pb-free and Sn/Pb solders.WF-9940 is very heat stable and well-suited for selective soldering applications. Even with the high degree of activation, WF-9940 passes all known reliability requirements. it is non-corrosive and does not contribute to detrimental circuit board insulation resistance degradation or electrochemical migration.Features:Compatible with Pb-free and Sn/Pb processesSuperior hole-fillPhysical Properties Color: AmberJ-STD-004 Flux Type: ROL1Information provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Specific Gravity 0.795 g/cc

@Temperature 25.0 °C
0.795 g/cc

@Temperature 77.0 °F
0.804 g/cc

@Temperature 15.5 °C
0.804 g/cc

@Temperature 59.9 °F
Solids Content 3.63 %
3.63 %
Thermal Properties Metric English Comments
Flash Point 12.2 °C
54.0 °F
TCC
Chemical Properties Metric English Comments
Acid Value 18
18
mgKOH/g flux
496
496
mgKOH/g flux solids