Industeel FORA 400 400 HB Wear Resistant Steel

Category Metal , Ferrous Metal , Carbon Steel , Medium Carbon Steel
Manufacturer Groupe Arcelor
Trade Name FORA
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Industeel FORA 400 400 HB Wear Resistant Steel.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: FORA 400 is a water quenched martensitic steel, with a typical hardness of 400HB (42.5 HRC), constituting a real answer to abrasive wear. Thanks to its toughness, its elevated hardness, its high yield strength, FORA 400 can be used wherever wear resistance to wear by sliding or by moderate impacts is required. Compared to conventional steels, such as S355, FORA 400 offers a real benefit to equipment life times and allows a significant thickness reduction in designs since its wear resistance is up to 3 times longer than S355 grade. Moreover, FORA 400 is very easily welded and has good forming properties thereby contributing to ease off fabrication. This steel is particularly suitable for applications in quarries, construction industry, mines, cement plants, iron and steel industry, etc.Information provided by manufacturer.
Mechanical Properties Metric English Comments
Hardness, Brinell 360 - 440
360 - 440
Typical
Hardness, Rockwell C 39 - 47
39 - 47
Typical
Tensile Strength, Ultimate 1350 MPa
196000 psi
Typical
Tensile Strength, Yield 1100 MPa
160000 psi
Typical
Elongation at Break 13 %
13 %
Typical
Charpy Impact 35.0 J

@Temperature -20.0 °C
25.8 ft-lb

@Temperature -4.00 °F
Typical
Component Elements Properties Metric English Comments
Carbon, C 0.20 %
0.20 %
Chromium, Cr 1.0 %
1.0 %
Iron, Fe 96.875 - 96.9 %
96.875 - 96.9 %
As remainder
Manganese, Mn 1.6 %
1.6 %
Molybdenum, Mo 0.30 %
0.30 %
Phosphorous, P <= 0.020 %
<= 0.020 %
Sulfur, S <= 0.0050 %
<= 0.0050 %