Industeel SUPERELSO® 890 HLE Steel for Welded and Weight-Saving Structures

Category Metal , Ferrous Metal , Carbon Steel , Medium Carbon Steel
Manufacturer Groupe Arcelor
Trade Name SUPERELSO®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Industeel SUPERELSO® 890 HLE Steel for Welded and Weight-Saving Structures.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: SUPERELSO® 890 is quenched and tempered steel for structure with higher strength. Thanks to a minimum yield strength of 890 N/mm² (130 KSI), SUPERELSO® 890 enables to make weight savings or support higher stresses and thus carry higher payload. With a good quality of steel making process, an adapted chemical analysis (low alloying content) and an excellent precision in Industeel's fabrication process (thickness tolerance, uniform mechanical characteristics), SUPERELSO® 890 is easy to machine, to bend and to weld which simplify production and maintenance. By using S SUPERELSO® 890 and thus thinner plate in welded structures, you limit preheating conditions, you decrease quantity of consumables, welding time and so production costs.Information provided by manufacturer.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 940 - 1100 MPa
136000 - 160000 psi
Typical
Tensile Strength, Yield >= 890 MPa

@Strain 0.200 %
>= 129000 psi

@Strain 0.200 %
Elongation at Break >= 11 %
>= 11 %
At 5%
13 %
13 %
Typical At 5%
Charpy Impact >= 30.0 J

@Temperature -20.0 °C
>= 22.1 ft-lb

@Temperature -4.00 °F
Transverse
>= 40.0 J

@Temperature -20.0 °C
>= 29.5 ft-lb

@Temperature -4.00 °F
Longitudinal
Component Elements Properties Metric English Comments
Aluminum, Al 0.040 - 0.070 %
0.040 - 0.070 %
Carbon, C 0.18 %
0.18 %
Chromium, Cr 0.80 %
0.80 %
Copper, Cu 0.30 %
0.30 %
Iron, Fe 93.91 - 93.94 %
93.91 - 93.94 %
As remainder
Manganese, Mn 1.5 %
1.5 %
Molybdenum, Mo 0.60 %
0.60 %
Nickel, Ni 2.0 %
2.0 %
Phosphorous, P 0.025 %
0.025 %
Silicon, Si 0.50 %
0.50 %
Sulfur, S 0.015 %
0.015 %
Vanadium, V 0.10 %
0.10 %