Charpy Impact >= 40.0 J

@Temperature -20.0 °C
>= 29.5 ft-lb

@Temperature -4.00 °F
Longitudinal
Industeel SUPERELSO® 960 HLE Steel for Welded and Weight-Saving Structures
Description: SUPERELSO® 960 is quenched and tempered steel for structure with higher strength. Thanks to a minimum yield strength of 960 N/mm² (140 KSI), SUPERELSO® 960 enables to make weig..
Charpy Impact >= 40.0 J

@Temperature -20.0 °C
>= 29.5 ft-lb

@Temperature -4.00 °F
Longitudinal
Industeel SUPRALSIM® 690 HLE Steel for Welded and Weight-Saving Structures
Description: SUPRALSIM® 690 is general steel plate for structure enables to make weight savings thanks to a minimum yield strength of 690 N/mm². Thanks to its exceptional purity rate (very low..
Charpy Impact 40.0 J

@Temperature -40.0 °C
29.5 ft-lb

@Temperature -40.0 °F
Longitudinal
ThyssenKrupp N-A-XTRA® 550 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..
Charpy Impact 40.0 J

@Temperature 0.000 °C
29.5 ft-lb

@Temperature 32.0 °F
Transverse
ThyssenKrupp N-A-XTRA® 550 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..
Charpy Impact 40.0 J

@Temperature -40.0 °C
29.5 ft-lb

@Temperature -40.0 °F
Longitudinal
ThyssenKrupp N-A-XTRA® 620 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..
Charpy Impact 40.0 J

@Temperature 0.000 °C
29.5 ft-lb

@Temperature 32.0 °F
Transverse
ThyssenKrupp N-A-XTRA® 620 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..
Charpy Impact 40.0 J

@Temperature -40.0 °C
29.5 ft-lb

@Temperature -40.0 °F
Longitudinal
ThyssenKrupp N-A-XTRA® 700 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..
Charpy Impact 40.0 J

@Temperature 0.000 °C
29.5 ft-lb

@Temperature 32.0 °F
Transverse
ThyssenKrupp N-A-XTRA® 700 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..
Charpy Impact 40.0 J

@Temperature -40.0 °C
29.5 ft-lb

@Temperature -40.0 °F
Longitudinal
ThyssenKrupp N-A-XTRA® 800 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied with a minimum yield strength of 800 MPa. It can ..
Charpy Impact 40.0 J

@Temperature 0.000 °C
29.5 ft-lb

@Temperature 32.0 °F
Transverse
ThyssenKrupp N-A-XTRA® 800 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied with a minimum yield strength of 800 MPa. It can ..
Charpy Impact 40.0 J

@Temperature -20.0 °C
29.5 ft-lb

@Temperature -4.00 °F
Longitudinal
ThyssenKrupp N-A-XTRA® M 550 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..
Charpy Impact 40.0 J

@Temperature -20.0 °C
29.5 ft-lb

@Temperature -4.00 °F
Longitudinal
ThyssenKrupp N-A-XTRA® M 620 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..
Charpy Impact 40.0 J

@Temperature -20.0 °C
29.5 ft-lb

@Temperature -4.00 °F
Longitudinal
ThyssenKrupp N-A-XTRA® M 700 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied in 3 different grades with a minimum yield streng..
Charpy Impact 40.0 J

@Temperature -20.0 °C
29.5 ft-lb

@Temperature -4.00 °F
Longitudinal
ThyssenKrupp N-A-XTRA® M 800 Structural Steel
This Material Specification applies to quenched and tempered heavy plates made of the special structural steel N-A-XTRA® This steel can be supplied with a minimum yield strength of 800 MPa. It can ..
Charpy Impact 40.0 J

@Temperature -20.0 °C
29.5 ft-lb

@Temperature -4.00 °F
Longitudinal
ThyssenKrupp XABO® 355 Structural Steel
This Material Specification applies to thermomechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-..
Charpy Impact 40.0 J

@Temperature -30.0 °C
29.5 ft-lb

@Temperature -22.0 °F
Longitudinal
ThyssenKrupp XABO® 500 T Structural Steel
This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-..
Charpy Impact 40.0 J

@Temperature -20.0 °C
29.5 ft-lb

@Temperature -4.00 °F
Longitudinal
ThyssenKrupp XABO® 890 Structural Steel
This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli..
Charpy Impact 40.0 J

@Temperature -20.0 °C
29.5 ft-lb

@Temperature -4.00 °F
Longitudinal
ThyssenKrupp XABO® 960 Structural Steel
This Material Specification applies to liquid-quenched and tempered heavy plates from 3 up to 100 mm in thickness, made of the high-strength special structural steels XABO® 890 and XABO® 960.Appli..
Charpy Impact 40.0 J

@Temperature -40.0 °C
29.5 ft-lb

@Temperature -40.0 °F
Longitudinal
ThyssenKrupp XABO® 355 T Structural Steel
This Material Specification applies to thermomechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-..
Charpy Impact 40.0 J

@Temperature -20.0 °C
29.5 ft-lb

@Temperature -4.00 °F
Longitudinal
ThyssenKrupp XABO® 500 Structural Steel
This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-..
Charpy Impact 40.0 J

@Temperature -20.0 °C
29.5 ft-lb

@Temperature -4.00 °F
Longitudinal
ThyssenKrupp XABO® 460 Structural Steel
This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-..
Charpy Impact >= 40.0 J

@Temperature -20.0 °C
>= 29.5 ft-lb

@Temperature -4.00 °F
Longitudinal
Industeel SUPERELSO® 890 HLE Steel for Welded and Weight-Saving Structures
Description: SUPERELSO® 890 is quenched and tempered steel for structure with higher strength. Thanks to a minimum yield strength of 890 N/mm² (130 KSI), SUPERELSO® 890 enables to make weight sav..
Charpy Impact 40.0 J

@Temperature -40.0 °C
29.5 ft-lb

@Temperature -40.0 °F
Longitudinal
ThyssenKrupp XABO® 460 T Structural Steel
This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-..
Charpy Impact >= 40.0 J

@Temperature -20.0 °C
>= 29.5 ft-lb

@Temperature -4.00 °F
Industeel CREUSABRO® 8000 High Performance Wear Resistant Steel
Description: CREUSABRO® 8000 is a high performance wear resistant steel, exhibiting a wear resistance of 50% higher than that of conventional 500 HB water quenched steel. CREUSABRO® 8000 is using ..