Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Industeel SUPERELSO® 960 HLE Steel for Welded and Weight-Saving Structures

Category Metal , Ferrous Metal , Carbon Steel , Medium Carbon Steel
Manufacturer Groupe Arcelor
Trade Name SUPERELSO®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Industeel SUPERELSO® 960 HLE Steel for Welded and Weight-Saving Structures.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: SUPERELSO® 960 is quenched and tempered steel for structure with higher strength. Thanks to a minimum yield strength of 960 N/mm² (140 KSI), SUPERELSO® 960 enables to make weight savings or support higher stresses and thus carry higher payload. With a good quality of steel making process, an adapted chemical analysis (low alloying content) and an excellent precision in Industeel's fabrication process (thickness tolerance, uniform mechanical characteristics), SUPERELSO® 960 is easy to machine, to bend and to weld which simplify production and maintenance. By using S SUPERELSO® 960 and thus thinner plate in welded structures, you limit preheating conditions, you decrease quantity of consumables, welding time and so production costs.Information provided by manufacturer.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 1000 - 1130 MPa
145000 - 164000 psi
Typical
Tensile Strength, Yield >= 960 MPa

@Strain 0.200 %
>= 139000 psi

@Strain 0.200 %
Elongation at Break >= 10 %
>= 10 %
13 %
13 %
Charpy Impact >= 30.0 J

@Temperature -20.0 °C
>= 22.1 ft-lb

@Temperature -4.00 °F
Transverse
>= 40.0 J

@Temperature -20.0 °C
>= 29.5 ft-lb

@Temperature -4.00 °F
Longitudinal
Component Elements Properties Metric English Comments
Aluminum, Al 0.040 - 0.070 %
0.040 - 0.070 %
Carbon, C 0.18 %
0.18 %
Chromium, Cr 0.80 %
0.80 %
Copper, Cu 0.30 %
0.30 %
Iron, Fe 93.91 - 93.94 %
93.91 - 93.94 %
As remainder
Manganese, Mn 1.5 %
1.5 %
Molybdenum, Mo 0.60 %
0.60 %
Nickel, Ni 2.0 %
2.0 %
Phosphorous, P 0.025 %
0.025 %
Silicon, Si 0.50 %
0.50 %
Sulfur, S 0.015 %
0.015 %
Vanadium, V 0.10 %
0.10 %