Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Industeel SUPRALSIM® 690 HLE Steel for Welded and Weight-Saving Structures

Category Metal , Ferrous Metal , Carbon Steel , Medium Carbon Steel
Manufacturer Groupe Arcelor
Trade Name SUPRALSIM®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Industeel SUPRALSIM® 690 HLE Steel for Welded and Weight-Saving Structures.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: SUPRALSIM® 690 is general steel plate for structure enables to make weight savings thanks to a minimum yield strength of 690 N/mm². Thanks to its exceptional purity rate (very low sulphur and phosphorous contents), and its adapted chemical analysis the SUPRALSIM® 690 steel is easy to shape and to weld.Information provided by manufacturer.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 770 - 940 MPa
112000 - 136000 psi
Tensile Strength, Yield >= 690 MPa

@Strain 0.200 %
>= 100000 psi

@Strain 0.200 %
Elongation at Break 14 %
14 %
Charpy Impact >= 30.0 J

@Temperature -20.0 °C
>= 22.1 ft-lb

@Temperature -4.00 °F
Transverse
>= 40.0 J

@Temperature -20.0 °C
>= 29.5 ft-lb

@Temperature -4.00 °F
Longitudinal
Component Elements Properties Metric English Comments
Aluminum, Al 0.020 - 0.050 %
0.020 - 0.050 %
Carbon, C 0.20 %
0.20 %
Chromium, Cr 1.2 %
1.2 %
Copper, Cu 0.50 %
0.50 %
Iron, Fe 93.88 - 93.91 %
93.88 - 93.91 %
As remainder
Manganese, Mn 1.6 %
1.6 %
Molybdenum, Mo 0.60 %
0.60 %
Nickel, Ni 1.35 %
1.35 %
Phosphorous, P 0.020 %
0.020 %
Silicon, Si 0.50 %
0.50 %
Sulfur, S 0.020 %
0.020 %
Vanadium, V 0.080 %
0.080 %