Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Ineos H12G-00 Polypropylene Homopolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos H12G-00 Polypropylene Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This is a general purpose homopolymer for injection molding applications. This material meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsGeneral purposeConsumer productsHousewaresRigid packagingInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Melt Flow 12.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 35.2 MPa

@Temperature 23.0 °C
5100 psi

@Temperature 73.4 °F
ASTM D638
Elongation at Break >= 200 %
>= 200 %
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 1.48 GPa

@Temperature 23.0 °C
215 ksi

@Temperature 73.4 °F
ASTM D790A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 82.2 °C
180 °F
ASTM D648
Descriptive Properties Value Comments
Process Injection Molding
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved