Ineos L70Z-01 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos L70Z-01 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
L70Z-01 is a nucleated and antistatic high flow polypropylene medium impact copolymer for injection molding applications. This product meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.Applications:Thin walled injection moldingClosuresBenefits:Enhanced impact & stiffnessImproved ProcessabilityAntistat includedInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Melt Flow 70 g/10 min

@Load 2.16 kg,
Temperature 230 °C
70 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.4 MPa
3400 psi
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790A
Izod Impact, Notched 0.694 J/cm

@Temperature -20.0 °C
1.30 ft-lb/in

@Temperature -4.00 °F
1/8" (3mm) notched bar; ASTM D256
1.39 J/cm

@Temperature 23.0 °C
2.60 ft-lb/in

@Temperature 73.4 °F
1/8" (3mm) notched bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 102 °C
216 °F
ASTM D648
Descriptive Properties Value Comments
Process Injection Molding