Thermal Properties | Metric | English | Comments |
---|---|---|---|
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics Cycoloy® C3650 PC+ABS (Asia Pacific) Flame retardant PC/ABS blend using non-brominated and non-chlorinated flame retardant systems, offering high impact and excellent extrusion and thermoforming characteristics. Halogen free according .. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | ASTM D648 |
Polymer Resources PPX-GP4-WR Modified-PPO, General Purpose, Wear Resistant Modified-Polyphenylene Oxide, General Purpose, Wear Resistant, 215F HDTProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test s.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | |
Eastman Eastalloy DA106 PC+PET Copolyester/Polycarbonate
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | 120°C/h; ISO 75/1 |
Polykemi AB POLYabs HD2 ABS Information provided by Polykemi AB |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | Edgew 120*10*4 sp=100mm; ISO 75/Be |
SABIC Innovative Plastics GELOY XP7560 ASA (Europe-Africa-Middle East) GELOY XP7560 is a general purpose ASA/PC injection moulding grade, available in various colours. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | |
Polimeri Europa SINKRAL B23 ABS, Heat Stabilized
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,105-04-16-25 High heat resistant grade with good impact resistance. Suitable for injection moulding and extrusi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | |
Arkema Group Oroglas® MI-4T Acrylic, Heat Resistant
(discontinued **) OROGLAS MI-4T is an acrylic grade that associates improved impact resistance with high heat resistance.Key features improved impact resistance: up to 4 times more impact resistant than standard acr.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | |
Ineos ABS Lustran® H605 Low emission, easy flowing.,Property data per ISO test methods. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ISO 75B |
Lucite International Diakon® CMG302 Acrylic Polymer Information provided by Lucite International |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C @Thickness 6.40 mm |
216 °F @Thickness 0.252 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics NORYL SE100X PPE+PS (Asia Pacific) Nonbrominated, nonchlorinated FR resin. Improved productivity and reliability. 199F HDT. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | Flatw 80*10*4 sp=64mm; ISO 75/Bf |
SABIC Innovative Plastics LNP LUBRICOMP ML004 PP LNP* LUBRICOMP* ML004 is a product based on Polypropylene containing 20% PTFE. Added features of this grade include: Wear Resistant. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® ABS 03010 Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel FiberFeatures: ESD Protection and Good MoldabilityInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® ABS SS5 FR 5% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 5% Filler by WeightFeatures: Electromagnetic Shielding (EMI) and Flame RetardantInformation provided by TP Compo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS GF10 LE 10% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 10% Filler by WeightFeatures: Low ExtractablesInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Techmer ES HiFill® ABS GF5 5% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 5% Filler by WeightInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | ASTM D648 |
Spartech PE4130 Reinforced High Density Polyethylene Compound Spartech Polycom's filled high molecular weight, high density polyethylenes are specifically designed for blow molding and sheet extrusion /thermoforming of structural parts. These materials offer a.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | ASTM D648 |
Spartech PP7120 Talc Filled High Impact Copolymer Good material choice for applications where low to medium levels of impact are required and where stiffness and heat deflection properties remain criticalInformation provided by Spartech |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C @Thickness 6.40 mm |
216 °F @Thickness 0.252 in |
ASTM D648 |
Samsung Cheil Industries Starex® VG-4910 ABS, Glass Filled FR Information provided by Samsung Cheil Industries. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® ABS SS15 BK MB 15% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 15% Filler by WeightFeatures: Electromagnetic Shielding (EMI)Appearance: BlackInformation provided by TP Composi.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | Unannealed; ASTM D648 |
Techmer ES Electrablend® ABS SS7 BK MB 7% Stainless Steel Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Stainless Steel Fiber, 7% Filler by WeightFeatures: ESD ProtectionAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C @Thickness 3.20 mm |
216 °F @Thickness 0.126 in |
unannealed; ASTM D648 |
SABIC Innovative Plastics LNP THERMOCOMP MB008S PP LNP* THERMOCOMP* MB008S is a compound based on Polypropylene resin containing 40% Glass Bead. Added features of this material include: Heat Stabilized. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ASTM D648 |
A. Schulman PP 1102-01 Polypropylene General Purpose, Molding Grade Polypropylene DescriptionPolypropylene PP 1102-01 is a general purpose, molding grade with UL 94 HB approval for use in large and thin wall applications. ApplicationPolypropylene PP 1102-01 meets FDA Regulation.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C @Thickness 3.20 mm |
216 °F @Thickness 0.126 in |
ISO 75 |
A. Schulman FORMION™ FI 232H 10% Mineral Reinforced Ionomer / Nylon Alloy DescriptionFormion® FI 232H is an injection molding grade, 10% mineral reinforced Ionomer / Nylon alloy, which has been formulated for high scratch resistance, high stiffness and exceptional impact.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 215 °F | ASTM D648 |
Washington Penn Homopolymer Polypropylene 30% Calcium Carbonate Filled Calcium carbonate-filled polypropylene compounds have been tailored specifically to meet the requirements of each of the major automobile producers. Grades are available to meet FDA food and drug pa.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ASTM D648 |
A. Schulman PP 3490-01G Polypropylene Homopolymer Polypropylene DescriptionPolypropylene PP 3490-01G Natural is a homopolymer for extrusion and compounding applications. This material can also be used as a carrier resin for color concentrates. ApplicationPP 349.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | Unannealed; ASTM D648 |
Dow NRD6-589 Polypropylene Random Copolymer Resin DOW NRD6-589 Polypropylene Resin is intended for use in injection molding applications. It offers excellent balance of impact and stiffness.Consistent processabilityGood stiffness/impact balanceGoo.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ASTM D648 |
A. Schulman ComAlloy Hiloy® 222 ABS, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.20% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 - 123 °C | 215 - 253 °F | Average value: 114 °C Grade Count:10 |
Overview of materials for Acrylic/Polycarbonate Alloy This property data is a summary of similar materials in the MatWeb database for the category "Acrylic/Polycarbonate Alloy". Each property range of values reported is minimum and maximum values of ap.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ASTM D648 |
A. Schulman PP 1102-01 Polypropylene General Purpose, Molding Grade Polypropylene DescriptionPolypropylene PP 1102-01 is a general purpose, molding grade with UL 94 HB approval for use in large and thin wall applications. ApplicationPolypropylene PP 1102-01 meets FDA Regulation.. |
|||
Deflection Temperature at 0.46 MPa (66 psi) | 102 °C | 216 °F | ASTM D648 |
Samyang Triel® 5550 Thermoplastics Polyetherester Elastomer, General Extrusion Excellent mechanical characteristics, elasticity, thermal resistance and chemical resistance.5550 is an extrusion grade.Information provided by Samyang. |