Material Notes:
Grade N00G-01 is a fractional melt flow rate impact copolymer for blow molding, pipe, tubing, and sheet extrusion. It offers a good balance of stiffness and impact strength as compared to other impact copolymers.
Physical Properties Metric English Comments
Melt Flow 0.50 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.50 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.3 MPa
3670 psi
2 in/min; ASTM D638
Flexural Modulus 1.14 GPa
165 ksi
ASTM D790A
Izod Impact, Notched 1.39 J/cm

@Temperature -20.0 °C
2.60 ft-lb/in

@Temperature -4.00 °F
ASTM D256
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 86.7 °C
188 °F
ASTM D648
Descriptive Properties Value Comments
Process Injection Molding
Pipe Extrusion
Sheet Extrusion
Region Mexico
Bamberger Polymers Distribution