Ineos N07N-00 Polypropylene Impact Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos N07N-00 Polypropylene Impact Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This is a medium melt flow rate, nucleated and antistatic impact copolymer polypropylene for injection molding applications that require a superior stiffness to impact balance.ApplicationsMaterials handlingConsumer productsBenefitsSuperior stiffness to impact balanceFast molding cycleGood mold releaseInformation provided by Ineos Olefins & Polymers USA
Physical Properties Metric English Comments
Melt Flow 7.2 g/10 min

@Load 2.16 kg,
Temperature 230 °C
7.2 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 22.1 MPa

@Temperature 23.0 °C
3200 psi

@Temperature 73.4 °F
ASTM D638
Elongation at Break >= 300 %
>= 300 %
ASTM D638
Flexural Modulus, 1% Secant 1280 MPa

@Temperature 23.0 °C
185000 psi

@Temperature 73.4 °F
0.05 in/min test speed
Izod Impact, Notched 1.33 J/cm

@Temperature -20.0 °C
2.50 ft-lb/in

@Temperature -4.00 °F
1/8'' notched bar; ASTM D256
NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
1/8'' notched bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
ASTM D648