Material Notes:
An antistated polypropylene random copolymer produced by Ineos utilizing unique catalyst technology. It is designed for blowmolding and extrusion applications and exhibits good stiffness and improved cycles. This material meets the Food and Drug Administration requirements of 21CFR 177.1520.
Physical Properties Metric English Comments
Density 0.898 g/cc
0.0324 lb/in³
ASTM D1505
Melt Flow 1.7 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.7 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 66
66
ASTM D2240
Tensile Strength, Ultimate 18.6 MPa
2700 psi
2 in/min.; ASTM D638
Tensile Strength, Yield 26.9 MPa
3900 psi
2 in/min (50 mm/min); ASTM D-638
Elongation at Break 550 %
550 %
2 in/min (50 mm/min); ASTM D-638
Elongation at Yield 10 %
10 %
2 in/min.; ASTM D638
Modulus of Elasticity 0.669 GPa
97.0 ksi
ASTM D638
Flexural Modulus 0.896 GPa
130 ksi
Secant @ 1% strain; ASTM D790
Izod Impact, Notched 0.430 J/cm
0.806 ft-lb/in
ASTM D256
Izod Impact, Unnotched >= 13.35 J/cm
>= 25.01 ft-lb/in
ASTM D256
Descriptive Properties Value Comments
Process Blow Molding/Extrusion