Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Modulus of Elasticity 0.669 GPa
97.0 ksi
ASTM D638
Ineos R01A-01 Polypropylene Copolymer, Antistatic
An antistated polypropylene random copolymer produced by Ineos utilizing unique catalyst technology. It is designed for blowmolding and extrusion applications and exhibits good stiffness and improv..
Modulus of Elasticity 0.669 GPa
97.0 ksi
Molded Sample 2% Secant Modulus
Dow HDPE 08454N High Density Polyethylene
DOW HDPE 08454N resin is a narrow molecular weight distribution copolymer designed to offer excellent impact strength and toughness, with good stiffness. This resin has good processability over a wi..
Modulus of Elasticity 0.669 GPa
97.0 ksi
Molded Sample 2% Secant Modulus
Dow HDPE 65053N High Density Polyethylene
DOW HDPE 65053N resin is a narrow molecular weight distribution copolymer designed to offer good environmental stress crack resistance and rigidity with high impact strength. This resin has excellen..