Ineos R35C-01 Polypropylene Random Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Ineos Olefins & Polymers USA
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ineos R35C-01 Polypropylene Random Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Grade R35C-01 is a high clarity random copolymer with a high flow rate. This material is designed for high speed injection molding and meets the requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520.ApplicationsConsumer products Housewares Medical Thin-wall rigid packagingBenefitsExcellent clarity High flow rate Rapid cycle times Good molding performance in thin-wall parts Good impact resistance at room and refrigerator temperatures
Physical Properties Metric English Comments
Melt Flow 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.7 MPa
4600 psi
ASTM D638
Flexural Modulus 1.31 GPa
190 ksi
ASTM D790B
Izod Impact, Notched 0.481 J/cm

@Diameter 3.17 mm
0.900 ft-lb/in

@Diameter 0.125 in
bar; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 87.8 °C
190 °F
ASTM D648
Optical Properties Metric English Comments
Haze 11 %

@Thickness 1.27 mm
11 %

@Thickness 0.0500 in
plaque; ASTM D1003
Descriptive Properties Value Comments
Process Injection Molding
Region Mexico
Bamberger Polymers Distribution