Material Notes:
Ineos T60-800 is a high density polyethylene homopolymer. This narrow molecular weight distribution resin is a product of Ineos' innovative technology. Parts fabricated from this material exhibit a glossy surface finish, and have good impact strength and rigidity. This material meets the Food and Drug Administration requirements of 21CFR 177.1520.
Physical Properties Metric English Comments
Density 0.961 g/cc
0.0347 lb/in³
ASTM D4883
Environmental Stress Crack Resistance 3.0 hour
3.0 hour
Condition B, 10%, F50; ASTM D1693
Melt Flow 8.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
8.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 31.0 MPa
4500 psi
2 in/min (50 mm/min); ASTM D-638
Elongation at Break >= 600 %
>= 600 %
2 in/min (50 mm/min); ASTM D-638
Flexural Modulus 1.552 GPa
225.1 ksi
Tangent-Method 1; ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 87.0 °C
189 °F
ASTM D648
Vicat Softening Point 128 °C
262 °F
ASTM D1525
Brittleness Temperature <= -75.0 °C
<= -103 °F
ASTM D746
Descriptive Properties Value Comments
Process Injection Molding
Region US & Canada
Bamberger Polymers Distribution