Inno-Comp INNOPOL® CS 5-8250 W 50% Chalk-Filled High Density Polyethylene

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene with 50% Calcium Carbonate , Polypropylene, Film Grade
Manufacturer Inno-Comp Ltd
Trade Name INNOPOL® CS
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Inno-Comp INNOPOL® CS 5-8250 W 50% Chalk-Filled High Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
INNOPOL® CS 5-8250 W is a 50% chalk-filled compound based on high density polyethylene.INNOPOL® CS 5-8250 W is developed for packaging film production.All information provided by INNO-COMP.
Physical Properties Metric English Comments
Density 1.46 g/cc

@Temperature 23.0 °C
0.0527 lb/in³

@Temperature 73.4 °F
ISO 1183
Melt Flow 0.35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
0.35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Elongation at Break, MD >= 250 %
>= 250 %
ISO 527
Film Elongation at Break, TD >= 100 %
>= 100 %
ISO 527
Elmendorf Tear Strength MD 12 g
12 g
ISO 6383-2
Elmendorf Tear Strength TD 140 g
140 g
ISO 6383-2
Dart Drop Test 20.0 g
0.0441 lb
ISO 7765
Film Tensile Strength at Break, MD 15.0 MPa
2180 psi
ISO 527
Film Tensile Strength at Break, TD 8.00 MPa
1160 psi
ISO 527
Descriptive Properties Value Comments
Color White