Iran Petrochemical (PCC) Arak 0410AA LLDPE  (discontinued **)

Category Polymer , Film , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Film Grade
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) Arak 0410AA LLDPE  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.924 - 0.928 g/cc
0.0334 - 0.0335 lb/in³
ASTM D1505
Melt Flow 0.90 - 1.1 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.90 - 1.1 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Film Tensile Strength at Yield, MD 12.0 MPa
1740 psi
ASTM D882
Film Tensile Strength at Yield, TD 13.0 MPa
1890 psi
ASTM D882
Film Elongation at Break, MD 650 %
650 %
ASTM D882
Film Elongation at Break, TD 850 %
850 %
ASTM D882
Dart Drop Test 90.0 g
0.198 lb
ASTM D1709
Film Tensile Strength at Break, MD 42.0 MPa
6090 psi
ASTM D882
Film Tensile Strength at Break, TD 33.0 MPa
4790 psi
ASTM D882
Thermal Properties Metric English Comments
Vicat Softening Point 105 °C
221 °F
ASTM D1525-75
Optical Properties Metric English Comments
Haze 13 %
13 %
ASTM D1003 A-61
Gloss 48 %
48 %
PU Meter, 45°C Head; ASTM D2456-70